MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Zenite® ZE55201 BK010 LCP
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), Mineral Filled

Material Notes: Zenite® ZE55201 BK010 is a 50% glass/mineral reinforced, lubricated, black liquid crystal polymer resin designed for ultra flatness.

Celenese acquired the Zenite product line from DuPont in 2010.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.85 g/ccISO 1183
Filler Content 50 %
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 88.0 MPaISO 527
Tensile Strength, Ultimate 76.0 MPa
@Temperature 23.0 °C
ASTM D 638
Elongation at Break 1.4 %ISO 527
 1.2 %
@Temperature 23.0 °C
ASTM D 638
Tensile Modulus 15800 MPaISO 527
Flexural Strength 136 MPaASTM D 790
 165 MPaISO 178
Flexural Modulus 12500 MPa
@Temperature 23.0 °C
ISO 178
 15400 MPa
@Temperature 23.0 °C
ASTM D 790
Charpy Impact, Notched 0.360 J/cm²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 175 VIEC 60112
 175 - 249 VUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear 13.0 µm/m-°C
@Thickness 4.00 mm,
Temperature -40.0 - 23.0 °C
ISO 11359-1/-2
 15.0 µm/m-°C
@Thickness 4.00 mm,
Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
 19.0 µm/m-°C
@Thickness 4.00 mm,
Temperature 160 - 250 °C
ISO 11359-1/-2
 20.0 µm/m-°C
@Thickness 4.00 mm,
Temperature 55.0 - 160 °C
ISO 11359-1/-2
CTE, linear, Transverse to Flow 25.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
ISO 11359-1/-2; 4mm
 27.0 µm/m-°C
@Thickness 4.00 mm,
Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
 34.0 µm/m-°C
@Thickness 4.00 mm,
Temperature 55.0 - 160 °C
ISO 11359-1/-2
 37.0 µm/m-°C
@Thickness 4.00 mm,
Temperature 160 - 250 °C
ISO 11359-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 278 °CASTM D 648
 290 °CISO 75-1/-2 1993/N2
UL RTI, Electrical 130 °C
@Thickness 0.800 mm
UL 746B
UL RTI, Mechanical with Impact 130 °C
@Thickness 0.800 mm
UL 746B
UL RTI, Mechanical without Impact 130 °C
@Thickness 0.800 mm
UL 746B
Flammability, UL94 V-0
@Thickness 0.800 mm
IEC 60695-11-10
 V-0
@Thickness 1.50 mm
IEC 60695-11-10
 V-0
@Thickness 1.50 mm
UL94
 V-0
@Thickness 0.800 mm
UL94
 V-0
@Thickness 3.00 mm
IEC 60695-11-10
 V-0
@Thickness 3.00 mm
UL94
 
Processing PropertiesOriginal ValueComments
Melt Temperature 335 °COptimum
 330 - 350 °C
Mold Temperature 80.0 °COptimum
 40.0 - 150 °C
Drying Temperature 150 °C
Dry Time 3 hourDehumidified Dryer
Moisture Content <= 0.010 %
 
Descriptive Properties
ColorBlack
Drying RecommendedYes
FillerGlass/Mineral
FormsPellets
GenericLCP
Part Marking Code>LCP-(GF+MD)50<ISO 11469
Polymer FamilyLCP
Polymer TypeLCP
Processing MethodInjection Molding
Product CategoryElectrical Resins
 Flame Retardant Resins
 Glass/Mineral Reinforced Resins
 Low Warp Resins
Region AvailableAmericas
 Asia/Pacific
 Europe
Resin IdentificationLCP-(GF+MD)50ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Therma-Tech™ LC-6000 TC Liquid Crystal Polymer (LCP)
Celanese ZENITE 5130L LCP, 30% Glass Reinforced
Celanese ZENITE 6130L LCP, 30% Glass Reinforced
Celanese ZENITE ZE55205 LCP, Specialty
Celanese Zenite® 6635 BK010 LCP

PDTA7792 / 89915

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.