MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Evonik DYNACOLL® Terra EO 480.01 Polyester-Polyol
Categories: Polymer; Renewable/Recycled Polymer; Thermoset; Polyester, TS

Material Notes: Bio-based Polyester-Polyols: With its DYNACOLL® Terra product range Evonik offers polyester-polyols made from renewable raw materials. These bio-based polyesters contain between > 30 and 100 ppw of renewable monomers. According to our DYNACOLL® 7000 product range a building block system of medium molecular weight copolyesters for moisture curing PUR hot melts was developed. It is divided in three basic groups:
  • Amorphous Grades
  • Liquid Grades
  • Crystalline Grades
DYNACOLL® Terra bio-based polyesters are usually supplied in 25 or 30 kg and 190 or 200 kg steel drums.

Your benefits:

  • support of resource efficiency by using green components
  • modular combination of polyesters in RHM formulation possible
  • available grades exhibiting broad range of properties in formulations
  • well-balanced and versatile adhesion properties
  • implementation of new properties possible

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity  2.0 cP
@Temperature 80.0 °C
2.0 cP
@Temperature 176 °F
DIN EN ISO 3219
 5.0 cP
@Temperature 130 °C
5.0 cP
@Temperature 266 °F
Reactive Hot Melt; DIN EN ISO 3219
Molecular Weight 3500 g/mol3500 g/mol
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 25.0 MPa3630 psiReactive Hot Melt
Elongation at Break 500 %500 %
 
Thermal PropertiesMetricEnglishComments
Melting Point 65.0 °C149 °F
Glass Transition Temp, Tg 20.0 °C68.0 °FDIN 53765
Ring & Ball Softening Point 70.0 °C158 °FReactive Hot Melt; DIN ISO 4625
 75.0 °C167 °FDIN ISO 4625
 
Descriptive Properties
Hydroxyl Number30 mg KOH/gDIN 53 240-02
Proportion of Renewables1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIL120 / 196324

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.