MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Taiyo America PSR-9000 FXT Series Liquid Photoimageable Solder Mask
Categories: Fluid

Material Notes: Liquid photoimageable dielectric material

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.387 g/cc
Viscosity 18000 - 22000 cP
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 213 kV/mm
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 80.2 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 900 - 1200 sec
 
Descriptive Properties
Binder SystemEpoxy
Dielectric TypeOrganic
Material TypeReady-To-Use Formulation

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SunChemical Gwent D2090126D2 Black Solder mask Dielectric
SunChemical Gwent D2090124D2 Green Solder mask Dielectric
Cadmium-Copper, Deoxidized, UNS C14300
AIM SAC305 Lead-Free Solder for Photonic Packaging
Dielectric Polymers NT-581 Fume Mask

PFLEXDM05 / 179279

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.