MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Chase Electronic Coatings HumiSeal® 1A33 Gel Urethane Conformal Coating
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: HumiSeal® 1A33 Gel conformal coating is: a thixotropic urethane gel, fast drying, single component. HumiSeal 1A33 Gel conformal coating has: excellent moisture and environmental protection for printed circuit assemblies, fluorescence under UV light for ease of inspection, no free isocyanates RoHS Directive 2002/95/EC compliance.

Information provided by Chase Electronic Coatings.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 44 %44 %± 2. By weight; Fed-Std-141, Meth. 4044
Volatile Organic Compounds (VOC) Content 521 g/l521 g/l
 
Processing PropertiesMetricEnglishComments
Cure Time  20.0 min
@Temperature 87.0 °C
0.333 hour
@Temperature 189 °F
Optimum Properties
 30.0 min
@Temperature 76.0 °C
0.500 hour
@Temperature 169 °F
Option
 43200 min
@Temperature 23.0 °C
720 hour
@Temperature 73.4 °F
Option
Tack-Free Time 10.2 min0.170 hourTo handle; Fed-Std-141, Meth. 4061

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHAS913 / 239774

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.