Molybdenum is alloyed with hafnium and carbon with extremely fine carbides providing a fine microstructure. Characteristics: - Outstanding heat resistance
- Outstanding creep resistance
- Withstands extreme thermal and mechanical loads
Typical Applications: Metal forming, extrusion dies Information provided by Plansee. |