MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Crosspolimeri TANEGUM ME/87 U2 Polyurethanes
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: TANEGUM: is the trade-mark of our modified polyurethanes technopolymers presenting many of the positive features of pure polyurethanes and improved capabilities of extrudibility.

TANEGUM ME/87 U2: they also have good resistance properties to flex-fatigue and to abrasion. They are suitable for electrical applications with resistance to ozone, hydrocarbons, oils, fats, fuels, and greases.

Information provided by Crosspolimeri S.P.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.23 g/ccASTM D792
Storage Temperature 12.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 84
@Time 15.0 sec
ASTM D2240
Tensile Strength 26.5 MPaASTM D638
 22.53 MPa
@Temperature 90.0 °C,
Time 605000 sec
Ageing in IRM 902 oil; IEC 60811
 26.5 MPa
@Temperature 100 °C,
Time 605000 sec
Heat Ageing; IEC 60811
Elongation at Break 450 %ASTM D638
 45 %
@Temperature 100 °C,
Time 605000 sec
Heat Ageing; IEC 60811
 337.5 %
@Temperature 90.0 °C,
Time 605000 sec
Ageing in IRM 902 oil; IEC 60811
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.50e+12 ohm-cmBS 6622
 
Thermal PropertiesOriginal ValueComments
Hot Ball Pressure Test 80.0 °C
@Time 14400 sec
16%, Penetration; IEC 60811
 
Processing PropertiesOriginal ValueComments
Zone 1 160 °C
Zone 2 165 °C
Zone 3 170 °C
Zone 4 180 °C
Die Temperature 175 - 180 °C
Head Temperature 170 - 175 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCROS142 / 294226

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.