MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Morgan Advanced Ceramics Bailey Bond Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Corundum. Bailey Bond Cement is a high conductivity filler which was originally developed to ensure good thermal contact between Bailey wall tiles and boiler tubing and provide an anti-corrosion coating layer. It is supplied as a putty consistency and should be kneaded into place to form a strong, heat conducting bond on drying and firing. Applications: Filler for good thermal contact between Bailey all tiles and boiler tubing.

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 2.16 W/m-K
@Temperature 600 °C
15.0 BTU-in/hr-ft²-°F
@Temperature 1110 °F
Maximum Service Temperature, Air <= 1000 °C<= 1830 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 76 %76 %
Fe2O3 3.0 %3.0 %
SiO2 16 %16 %
 
Descriptive Properties
Water Additionready mixed, 25 kg bag weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aremco Ceramabond™ 685
BASF Ultradur® B 4300 G2 10% Glass Filled PBT
Overview of materials for Nylon 66, Impact Grade
BASF Capron® HPN 9233G HS BK-102 33% Glass-Filled Nylon 6 (Dry)

CMORF6172 / 202956

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.