MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

SABIC LNP™ THERMOCOMP™ AF004XXY ABS (Americas)  (Unverified Data**)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: LNP THERMOCOMP AF004XXY is a compound based on ABS containing 20% glass fiber.

Information provided by SABIC Innovative Plastics for the Americas.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccASTM D 792
Density 1.19 g/cc0.0430 lb/in³ISO 1183
Moisture Absorption 0.250 %
@Time 86400 sec
0.250 %
@Time 24.0 hour
50% RH; ASTM D 570
Linear Mold Shrinkage, Flow  0.0020 cm/cm
@Time 86400 sec
0.0020 in/in
@Time 24.0 hour
ASTM D 955
 0.0020 cm/cm
@Time 86400 sec
0.0020 in/in
@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse  0.0040 cm/cm
@Time 86400 sec
0.0040 in/in
@Time 24.0 hour
ASTM D 955
 0.0040 cm/cm
@Time 86400 sec
0.0040 in/in
@Time 24.0 hour
ISO 294
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 76.0 MPa11000 psiType I, 5 mm/min; ASTM D 638
 77.0 MPa11200 psi5 mm/min; ISO 527
Elongation at Break 1.8 %1.8 %5 mm/min; ISO 527
 2.0 %2.0 %Type I, 5 mm/min; ASTM D 638
Tensile Modulus 6.04 GPa876 ksi1 mm/min; ISO 527
 6.08 GPa882 ksi50 mm/min; ASTM D 638
Flexural Strength 119 MPa17300 psiISO 178
 122 MPa17700 psi1.3 mm/min, 50 mm span; ASTM D 790
Flexural Modulus 5.97 GPa866 ksi2 mm/min; ISO 178
 6.08 GPa882 ksi1.3 mm/min, 50 mm span; ASTM D 790
Izod Impact, Notched 0.800 J/cm
@Temperature 23.0 °C
1.50 ft-lb/in
@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 3.74 J/cm
@Temperature 23.0 °C
7.01 ft-lb/in
@Temperature 73.4 °F
ASTM D 4812
Izod Impact, Notched (ISO) 7.00 kJ/m²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 23.0 kJ/m²
@Temperature 23.0 °C
10.9 ft-lb/in²
@Temperature 73.4 °F
80*10*4; ISO 180/1U
Impact Test 2.00 J1.48 ft-lbMultiaxial Impact; ISO 6603
Instrumented Impact Total Energy 13.0 J
@Temperature 23.0 °C
9.59 ft-lb
@Temperature 73.4 °F
ASTM D 3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 56.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
31.1 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D 696
CTE, linear, Transverse to Flow 52.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
28.9 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D 696
Deflection Temperature at 1.8 MPa (264 psi) 100 °C212 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 100 °C
@Thickness 3.20 mm
212 °F
@Thickness 0.126 in
unannealed; ASTM D 648

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI46871 / 187956

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.