MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Evonik VESTAMID® DX9380 NC Nylon 612
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612); Nylon 612, Unreinforced

Material Notes: VESTAMID® DX9380 NC is an impact modified resin based on polyamide 612 that is exclusively used as innermost layer in Evonik low extractable Multilayer Tubes like MLT 4800. VESTAMID® DX9380 NC offers outstanding properties concerning low extractables in fuel contact and a good impact resistance at low temperatures. VESTAMID® DX9380 NC is supplied as cylindrical granules, ready for processing, in moisture-proof bags. Pigmentation may affect values. Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.
Dry properties listed below
Industrial Sector: Automotive and Mobility, Sustainable
Sustainability: Sustainable electricity
Processing: Injection molding, , Extrusion
Delivery form: Pellets, Granules
Additives: Release agent, Unfilled
Applications: Tube and hose
Processing: Pipe/Tube extrusion
Special Characteristics: High impact strength, Light-stabilized, High heat resistant, Low extractables
Additives: Release agent, Impact resistant

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ISO 1183
Viscosity Number 220 cm³/g2.20 dl/gISO 307, 1157, 1628
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 42.0 MPa6090 psiISO 527
Tensile Strength 48.0 MPa6960 psiISO 527
Tensile Stress 41.0 MPa
@Strain 50.0 %
5950 psi
@Strain 50.0 %
ISO 527
Tensile Strength, Yield 48.0 MPa6960 psiISO 527
Elongation at Break >= 50.0 %>= 50.0 %Nominal; ISO 527
Elongation at Yield 6.00 %6.00 %ISO 527
Tensile Modulus 1.80 GPa261 ksiISO 527
Charpy Impact, Notched 4.10 J/cm²19.5 ft-lb/in²Type of failure: C; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 212 °C414 °FISO 11357-1/-3
 
Processing PropertiesMetricEnglishComments
Moisture Content 0.0300 %0.0300 %ISO 15512
 
Descriptive Properties
Blue water consumption22.2 kgISO 14040, 14044
Global Warming Potential2.4 kg CO2 eq./kgsavings incl. bio. C. as compared to classical production, ISO 14040, 14044
 6.9 kg CO2 eq./kgincl. bio. C incl. LUC, ISO 14040, 14044
 6.9 kg CO2 eq./kgexcl. bio. C incl. LUC, ISO 14040, 14044
Land use (ReCiPe 2016)0.3 Annual crop eq. yISO 14040, 14044
Weight per 1000 granules15.9 g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIK7897 / 325029

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.