MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Industeel SOLEIL C5 13% Cr 4 Ni Martensitic Stainless Steel with Improved Toughness
Categories: Metal; Ferrous Metal; Martensitic; Stainless Steel; T S40000 Series Stainless Steel

Material Notes: Description: Soleil C5 is a 13% Cr 4 Ni 0.5 Mo martensitic stainless steel. Its nickel content, associated with low carbon ensures better weldability, ductility, impact resistance and fatigue resistance properties when compared to 13 Cr ferritic-martensitic grades (AISI 410-420/Euronorms 1.4000 X6 Cr 13). The alloy has good corrosion resistance to fresh water and performs well under erosion-corrosion phenomena. The alloy is specially designed for all applications requiring high mechanical properties combined with high toughness and may be used in medium corrosive conditions. Typical applications are shafts or compressor impellers, particularly for hydraulic applications.

Information provided by manufacturer.

Key Words: EURONORM 1.4313-X4 Cr Ni Mo 13-4, AFNOR Z4 CN13.4, DIN X5 Cr Ni 13-4 W.Nr. 1.4313, AISI 41500
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.70 g/cc0.278 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 220 - 320220 - 320Typical
Tensile Strength, Ultimate 750 - 950 MPa109000 - 138000 psiMinimum Guaranteed
Tensile Strength, Yield >= 560 MPa>= 81200 psiMinimum Guaranteed
 >= 580 MPa
@Strain 1 %
>= 84100 psi
@Strain 1 %
Elongation at Break >= 18 %>= 18 %
Modulus of Elasticity 206 GPa29900 ksi
Poissons Ratio 0.2880.288Calculated
Shear Modulus 80.0 GPa
@Temperature 20.0 °C
11600 ksi
@Temperature 68.0 °F
Charpy Impact >= 80.0 J>= 59.0 ft-lb
 100 J73.8 ft-lbTypical
 >= 60.0 J
@Temperature 0.000 °C
>= 44.3 ft-lb
@Temperature 32.0 °F
 80.0 J
@Temperature 0.000 °C
59.0 ft-lb
@Temperature 32.0 °F
Typical
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000800 ohm-cm
@Temperature 20.0 °C
0.0000800 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.0 µm/m-°C
@Temperature 0.000 - 100 °C
6.11 µin/in-°F
@Temperature 32.0 - 212 °F
 12.0 µm/m-°C
@Temperature 0.000 - 400 °C
6.67 µin/in-°F
@Temperature 32.0 - 752 °F
Specific Heat Capacity 0.460 J/g-°C
@Temperature 20.0 °C
0.110 BTU/lb-°F
@Temperature 68.0 °F
Thermal Conductivity 26.0 W/m-K
@Temperature 20.0 °C
180 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.040 %0.040 %
Chromium, Cr 13 %13 %
Iron, Fe 82.039 %82.039 %As remainder
Molybdenum, Mo 0.50 %0.50 %
Nickel, Ni 4.0 %4.0 %
Phosphorus, P 0.020 %0.020 %
Silicon, Si 0.40 %0.40 %
Sulfur, S 0.0010 %0.0010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Outokumpu 4313 Martensitic Stainless Steel
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Annealed
CA6NM Martensitic Stainless Steel, Annealed Bar, Forgings, UNS S41500
410 Stainless Steel
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1150M (Heated 760°C/2hr/AC then 621°C/4hr/AC)

NINDUST19 / 17557

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.