MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

TPI Porene® ABS-GA850 High Impact ABS Resin
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded

Material Notes: Information provided by US distributor Polymer Technology and Services, LLC (PTS).

Key Words: Poly(Acrylonitrile Butadiene Styrene); Thai Petrochemical Industry; Polymer Technology & Services, LLC (PTS)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ASTM D792
Melt Flow 20 g/10 min
@Load 10.0 kg,
Temperature 220 °C
20 g/10 min
@Load 22.0 lb,
Temperature 428 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 118118ASTM D785
Tensile Strength, Yield 51.7 MPa
@Thickness 3.17 mm
7500 psi
@Thickness 0.125 in
Flexural Yield Strength 70.3 MPa
@Thickness 3.17 mm
10200 psi
@Thickness 0.125 in
Flexural Modulus 2.34 GPa
@Thickness 3.17 mm
339 ksi
@Thickness 0.125 in
Izod Impact, Notched  2.67 J/cm
@Thickness 6.35 mm
5.00 ft-lb/in
@Thickness 0.250 in
 2.99 J/cm
@Thickness 3.17 mm
5.60 ft-lb/in
@Thickness 0.125 in
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 96.0 °C205 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 87.0 °C189 °FASTM D648
Flammability, UL94  HB
@Thickness 1.59 mm
HB
@Thickness 0.0625 in
 HB
@Thickness 3.17 mm
HB
@Thickness 0.125 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 193 °C380 °F
Middle Barrel Temperature 216 °C420 °F
Front Barrel Temperature 232 °C450 °F
Melt Temperature 218 - 260 °C425 - 500 °FNozzle temp not greater than stock
Mold Temperature 48.9 - 65.6 °C120 - 150 °F
Drying Temperature 87.8 - 93.3 °C190 - 200 °F
Dry Time 2 - 24 hour2 - 24 hour
Injection Pressure 68.9 - 82.7 MPa10000 - 12000 psi
Back Pressure 0.689 MPa100 psi
Screw Speed 50 - 60 rpm50 - 60 rpm
 
Descriptive Properties
Injection Fill SpeedSlow to Moderate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsui TPX® RT18 Methylpentene Copolymer, Transparent Grade
TPI Porene® ABS-SR101 High Impact Extrusion Grade ABS Resin
TPI Porene® ABS-SP-100 Super High Impact ABS Resin
TPI Porene® ABS-GA800 High Impact ABS Resin
IRPC Polimaxx Porene SR101 Acrylonitrile Butadiene Styrene

PLBT03 / 50499

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.