MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
PoolKemie POLIMOLD HR 30 Polyurethane fluid rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Introduction: Two component room temperature vulcanizing fluid rubber which cures after addition and mixing with the appropriate catalyst: it produces an elastic and tenacious mass, free from bubbles and imperfections; it has a good stability to hydrolysis, very good mechanical resistance, is easy to demould and has a percent shrinkage approx. = 0. Poly-urethane rubbers of POLIMOLD HR series, once cured, have a light superficial greasiness caused by proper release agents in order to favor demoulding operations.

Application: Low and medium hardness types (HR 25 – 30) are suitable for reproduction of complex patterns with undercuts; high hardness types are specially suited for reproduction of large-sized patterns. Moulds made of POLIMOLD HR are suitable for mass-production plaster and cement handworks, for artistic foundry (loosewax method), in wax industry (decorative candles).

Information provided by Poolkemie

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.00 g/ccmixture A+B
Viscosity 800 - 1000 cPmixture A+B
Linear Mold Shrinkage <= 0.010 cm/cmafter 5 days ageing; ISO 4823
Storage Temperature 5.00 - 30.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 27 - 33
Elongation at Break >= 1000 %
Tear Strength 40.0 - 46.0 kN/mDIN 53515
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 hourDemoulding time
 72.0 hourHardening time
Pot Life 20.0 minmixture A+B
Shelf Life 8.00 MonthBoth components (A and B) in their original tightly closed containers, in a dry and cool place , away from moisture
 
Descriptive Properties
Mixing ratio100:100mixture A+B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPOOLK023 / 318502

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.