MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Versalis Riblene® MP 31 Low Density Polyethylene - Injection Molding
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Molded

Material Notes: Riblene MP 31 is a medium fluidity low density polyethylene resin (LDPE), with added slip agent.

Parts made by Riblene MP 31 are characterized by a medium rigidity.

Main Applications: Riblene MP 31 is suitable for injection molding and compound applications. Riblene MP 31 is recommended for caps, stoppers, closures and medium thickness articles.

Information provided by Polimeri Europa.

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.924 g/ccISO 1183
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 50ISO 868/A
Tensile Strength, Yield 12.0 MPaISO 527
Flexural Modulus 200 MPaISO 178
 
Thermal PropertiesOriginal ValueComments
Melting Point 112 °CInternal method
Vicat Softening Point 92.0 °C
@Load 1.00 kg
ISO 306/A
Brittleness Temperature <= -65.0 °CASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Versalis Riblene® MM 20 Low Density Polyethylene - Injection Molding
Versalis Riblene® MP 31 R Low Density Polyethylene - Injection Molding
Versalis Riblene® MM 20 R Low Density Polyethylene - Injection Molding
Versalis Riblene® MP 20 Low Density Polyethylene - Injection Molding
Versalis Riblene® MP 30 Low Density Polyethylene - Injection Molding

PENG033 / 124427

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.