MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Aperam Nicrimphy® 800 Cold Rolled Strip
Categories: Metal; Ferrous Metal

Material Notes: Nicrimphy 800 is a Nickel-Chromium alloy used when resistance to oxidation, carburization and other type of high temperature corrosion is needed. Nicrimphy 800 presents a good corrosion resistance to many aqueous media and a good resistance to stress corrosion cracking. Nicrimphy 800 is used for electrical heating elements, furnace components and equipments, heat exchangers, cracking tubes.

International standards: Werkstoff Nr 1.4876 - ASTM B409 – ASTM A240 and UNS N08800 – AMS 5871

Information provided by Aperam

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.00 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 150Annealed
Tensile Strength 600 MPaAnnealed
Tensile Strength, Yield 250 MPaAnnealed
Elongation at Break 35 %Annealed
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.000099 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 15.0 µm/m-°C
@Temperature 20.0 - 100 °C
Specific Heat Capacity 0.500 J/g-°C
Thermal Conductivity 13.0 W/m-K
Melting Point 1370 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.15 - 0.60 %
Chromium, Cr 19 - 23 %
Iron, Fe >= 39.5 %
Nickel, Ni 30 - 34 %
Titanium, Ti 0.15 - 0.60 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 1006 Steel, CQ, DQ, and DQSK sheet, 1.6-5.8 (0.06-0.23 in) mm thick
AISI 1012 Steel, CQ sheet,1.6-5.8 mm round or thickness
AISI 1010 Steel, hot rolled bar, 19-32 mm (0.75-1.25 in) round or thickness
AISI 1010 Steel, CQ sheet,1.6-5.8 mm round or thickness
AISI 1008 Steel, hot rolled bar, 19-32 mm (0.75-1.25 in) round

NPERA037 / 194826

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.