MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Universal Wire Works 347 Stainless Steel (AMS 5680) Filler Metal
Categories: Metal; Ferrous Metal; Stainless Steel

Material Notes: Universal 347 is extensively used with the gas tungsten arc, gas metal arc and submerged arc processes. This alloy is suitable for welding stabilized steel grades 321, 347 and 348. Alloy 347 should be used when high service temperatures are encountered (above 700°F). Alloy 347 is similar to type 321, but has a higher creep strength. Excellent for aircraft exhaust components.

Information provided by Universal Wire Works for their line of welding wire and filler metal.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 621 MPa90000 psi
Tensile Strength, Yield 414 MPa
@Strain 0.2 %
60000 psi
@Strain 0.2 %
Elongation at Break 40 %40 %
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.060 %0.060 %
Chromium, Cr 20 %20 %
Iron, Fe >= 54.6 %>= 54.6 %As Remainder
Manganese, Mn 1.8 %1.8 %
Molybdenum, Mo <= 0.75 %<= 0.75 %
Nb + Ta 12 %12 %
Nickel, Ni 10 %10 %
Phosphorus, P 0.020 %0.020 %
Silicon, Si 0.75 %0.75 %
Sulfur, S 0.010 %0.010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
347 Stainless Steel, annealed
Titanium Grade 1
Universal Wire Works 321 Stainless Steel (AMS 5689) Filler Metal
Aluminum 2024-T3
Aluminum 2024-T4; 2024-T351

NUWW274 / 19723

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.