MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
RAMPF RAKU® TOOL InnoClear™ OC-5313 Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Water-clear, semi-rigid polyurethane formulated

Key Properties:

  • Excellent physical properties after RT cure
  • Free of mercury, MOCA or TDI
  • Excellent optical clarity as well as U.V. stability
Applications:
  • For room temperature hand-batch or vacuum assisted casting methods
Cure 1: 24 hours at 77°F + 16 hours at 175°F
Cure 2: 7 days at 77°F

Information provided by © RAMPF Tooling Solutions GmbH & Co. KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.07 g/ccHardener; ASTM D-792
 1.07 g/ccCure 1; ASTM D-792
 1.07 g/ccCure 2; ASTM D-792
 1.08 g/ccResin; ASTM D-792
Viscosity 225 cPMix; ASTM D-2393
 250 cPResin; ASTM D-2393
 550 cPHardener; ASTM D-2393
Linear Mold Shrinkage 0.0010 - 0.0040 in/inCure 1; ASTM D-2566
 0.0010 - 0.0040 in/inCure 2; ASTM D-2566
Storage Temperature 15.0 - 30.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 75 - 89Cure 1; ASTM D-2240
 75 - 89Cure 2; ASTM D-2240
Tensile Strength 5500 psiCure 2; ASTM D-638
 6100 psiCure 1; ASTM D-638
Elongation at Break 16 %Cure 1; ASTM D-638
 17 %Cure 2; ASTM D-638
Flexural Strength 8500 psiCure 2; ASTM D-790
 10000 psiCure 1; ASTM D-790
Flexural Modulus 230000 psiCure 2; ASTM D-790
 250000 psiCure 1; ASTM D-790
Izod Impact, Notched 1.20 ft-lb/inCure 2; ASTM D-256
 1.50 ft-lb/inCure 1; ASTM D-256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 55.0 °CCure 2; ASTM D-648
 79.0 °CCure 1; ASTM D-648
 
Processing PropertiesOriginal ValueComments
Cure Time 6.00 - 8.00 hourMix, Demold time
Gel Time 20.0 - 30.0 minMix
 
Descriptive Properties
AspectWater ClearCure 1
 Water ClearCure 2
Mix Ratio100:100Resin: Hardener, Volume
 100:99Resin: Hardener, Weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PRAMPF132 / 317732

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.