MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

NOVA Chemicals NOVAPOL® TF-Y882-BP LLDPE Film Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes:

Hexene Copolymer

Features:

  • Good stiffness and machinability
  • Exceptional toughness
  • Suitable for narrow die gaps

Additives:

  • Processing antioxidant
  • Polymer process aid
  • Slip (750 ppm)
  • Antiblock (3150 ppm)

Applications:

  • Industrial packaging
  • High strength liners

Film properties are typical of blown film extruded on a 2.5" extruder with 4" die and 35-mil die gap at a blow up ratio of 2.5:1, but are dependent upon operating conditions.

United States: NOVAPOL TF-Y822 Series resin complies with the specifications contained in the U.S. Food and Drug Administration (FDA) regulation 21 CFR 177.1520 for olefin polymers, para. (c) 3.2a, and may thus be used in the United States as an article or component of an article intended for use in contact with food, without temperature or food-type restrictions, subject to technical suitability.

NOVA Chemicals polyethylene resins are biologically and chemically inert.

Information provided by NOVA Chemicals®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.921 g/cc0.0333 lb/in³ASTM D 792
Thickness 25.0 microns0.984 mil
Melt Index of Compound 0.80 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.80 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 12.0 MPa1740 psiASTM D 882
Film Tensile Strength at Yield, TD 12.0 MPa1740 psiASTM D 882
Film Elongation at Break, MD 560 %560 %ASTM D 882
Film Elongation at Break, TD 810 %810 %ASTM D 882
Elmendorf Tear Strength MD 350 g350 gASTM D 1922
Elmendorf Tear Strength TD 540 g540 gASTM D 1922
Dart Drop Test 130 g0.287 lbF50; ASTM D 1709/A
Film Tensile Strength at Break, MD 49.0 MPa7110 psiASTM D 882
Film Tensile Strength at Break, TD 42.0 MPa6090 psiASTM D 882
1% Secant Modulus, MD 120 MPa17400 psiASTM D 882
1% Secant Modulus, TD 280 MPa40600 psiASTM D 882
 
Optical PropertiesMetricEnglishComments
Haze 13 %13 %ASTM D 1003
Gloss 53 %53 %@ 45°; ASTM D 2457
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
Low Friction Puncture (J/mm)43NOVA Chemicals test method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOVB042 / 194650

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.