MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Dow SRD7677 Polypropylene Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: DOW SRD7677 is intended for use in injection molding processes. It is especially suited for thin-wall/long flow path molds.

Information provided by Dow

Braskem acquired Dow's polypropylene business. This specific grade was discontinued priot to the acquisition and so is listed as a discontinued Dow product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D792
Melt Flow 35 g/10 min
@Temperature 230 °C
35 g/10 min
@Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 21.8 MPa3160 psimolded and tested in accordance with ASTM D 4101; ASTM D638
Elongation at Yield 4.0 %4.0 %molded and tested in accordance with ASTM D 4101; ASTM D638
Flexural Modulus, 1% Secant 1100 MPa159000 psimolded and tested per ASTM D 4101; ASTM D790A
Izod Impact, Notched 1.01 J/cm1.90 ft-lb/inmolded and tested in accordance with ASTM D 4101; ASTM D256A
Gardner Impact 15.4 J
@Temperature -30.0 °C
11.3 ft-lb
@Temperature -22.0 °F
molded and tested in accordance with ASTM D 4101; ASTM D5420GC
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 98.9 °C210 °Funannealed; molded and tested in accordance with ASTM D 4101; ASTM D648

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow NRD6-589 Polypropylene Random Copolymer Resin
ExxonMobil PP3155E3 Polypropylene Copolymer
ExxonMobil ExxonMobil™ AXO3BE3 Polypropylene Impact Copolymer
ExxonMobil AXO3BE3 Impact Copolymer
ExxonMobil ACHIEVE 1605 Exxpol Metallocene Grade for Injection Molding Applications

PDOW1294 / 30512

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.