MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Konson CBS Rubber Accelerator
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Chemical Name: N-cyclohexyl-2-benzothiazole Sulfenamide

Molecular Formula: C13H16N2S2

CAS#: 95-33-0

Properties: Density :1.31~1.34g/cm3 ,Soluble in benzene and ethyl acetate, insoluble in water, slightly soluble in gasoline.

Applications: A good delayed action accelerator, suitable for natural and synthetic rubber and tire rubber products, able to improve the physical and mechanical properties of rubber products. CBS is regulated for use in articles in contact with food as specified under FDA 21 CFR177.2600 and under BgVV XXI, Category 4.

Information provided by Konson®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.31 - 1.34 g/cc0.0473 - 0.0484 lb/in³
Molecular Weight 264.4 g/mol264.4 g/mol
Ash <= 0.20 %<= 0.20 %
 
Thermal PropertiesMetricEnglishComments
Melting Point >= 99.0 °C>= 210 °FInitial
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
AppearanceGrey-white or Light-yellow Powder or granule
Heat Loss<0.2%
Sieve residue0150µm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKONS042 / 256087

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.