MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lanxess LEWATIT® ASB 1 Styrene/DVB Anion Exchange Resin
Categories: Polymer; Thermoset

Material Notes: Lewatit® ABS 1 is a premium grade, gel, strong base, Type 1, anion exchange resin based on a styrene/DVB polymer. Lewatit ASB 1 is especially suited for high purity separate bed, or mixed bed applications, where silica reduction in the final treated water is a critical requirement. Lewatit ASB 1 exhibits a high ion exchange capacity combined with excellent mechanical and osmotic strength for a long operating life. Lewatit ASB 1 is supplied in a heterodispersed particle size distribution as spherical beads in the fully swollen moist bead form. Lewatit ASB 1 is prepared with a minimum amount of fines (-50 mesh particles) resulting in low pressure losses during service. Lewatit ASB 1 OH is supplied in the hydroxide form. It is also available in its hydroxide form, designated as Lewatit ASB 1 OH.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.704 g/cc0.0254 lb/in³
Density 1.12 g/cc0.0405 lb/in³
Bead Size 0.300 - 1.25 mm0.0118 - 0.0492 in>90%
Storage Temperature -20.0 - 40.0 °C-4.00 - 104 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 71.0 °C160 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
AppearanceTranslucent
pH Operating Range0 - 14

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY8736 / 209129

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.