MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Saint-Gobain Norton® Fluorglas® Chemfilm® R167 Extruded Expanded PTFE Film (0.010" thick)
Categories: Polymer; Film; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Molded

Material Notes: Description: Expanded Unsintered Films are used in microwave and coaxial cable applications in which low dielectric constant and high velocities are required. R167-nominal density of 0.7 g/cc. R165-nominal density of 0.5 g/cc. PTFE = polytetrafluoroethylene
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.700 g/cc0.700 g/ccASTM D-792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 1.03 MPa150 psiTransverse/Width
 11.7 MPa1700 psiLongitudinal
Elongation at Break 125 %125 %ASTM D-882

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
W. L. Gore GORE™ 800 PTFE Universal Pipe Gasket (Style 800)
Arkema Rilsamid® AESNO MED Nylon 12
3M Dyneon™ TF 2021 PTFE
3M 5498 PTFE Film Tape
Saint-Gobain CHR® 2045-5 Skived PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape

PSTGQZ140 / 68654

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.