MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Palm Labs Adhesives TURBO SEAL SERIES 80 WHITE GENERAL PURPOSE THREAD SEALANT
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: TURBO SEAL SERIES 80 is a high performance control strength anaerobic thread sealant designed for the locking and sealing of metal threaded pipes and fittings.

NSF Certified Certified to ANSI/NSF Standard 61 for use in commercial and residential potable water systems not exceeding 82° C.

UL Classification Classified as small fire hazard. No flash point in liquid state. Ignition temperature 465°C. For use in devices handling gasoline, petroleum oils, natural gas, propane and butane.

Pressure Resistance TURBO SEAL SERIES 80 was successfully tested for pressure resistance and sealability to 3,000 psi 3/8” NPT steel pipe tees and plugs were assembled and pre-torqued to 27 N.m and allowed to cure 24 hours prior to testing at 3,000 psi hydraulic pressure according to ASTM D 1599.

Part Numbers for this data: 80-051, 80-251, 80-300, 80-1000, 80-2000

Information provided by Palm Laboratories Adhesives

Key Words: CAS No: 25852-47-5, 9004-96-0, 112945-52-5, 80-15-9, 57-55-6 and 9002-84-0
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/cc
Brookfield Viscosity 300000 cPRVT Spindle 3 @ 20 rpm
 
Mechanical PropertiesOriginal ValueComments
Shear Strength >= 1.00 MPaSteel Pins & Collars; ISO 10123
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°CASTM D696
Specific Heat Capacity 0.300 J/g-°C
Thermal Conductivity 0.100 W/m-KASTM C177
Maximum Service Temperature, Air 300 °C
Minimum Service Temperature, Air -65.0 °C
Flash Point >= 100 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 0.167 - 0.500 hourHandling
 2.00 - 4.00 hourFunctional
 24.0 hourFull
 
Descriptive Properties
AppearanceWhite
Chemical Resistance100% Initial Strength RetainedMotor Oil at 125°C, at 500hrs
 100% Initial Strength RetainedGasoline at 22°C, at 500hrs
 100% Initial Strength RetainedBrake Fluid at 22°C, at 500hrs
 100% Initial Strength RetainedWater/Glycol at 87°C, at 500hrs
 85% Initial Strength RetainedAcetone at 22°C, at 1000hrs
 90% Initial Strength RetainedEthanol at 22°C, at 1000hrs
 90% Initial Strength RetainedAcetone at 22°C, at 500hrs
 90% Initial Strength RetainedEthanol at 22°C, at 500hrs
 90% Initial Strength RetainedWater/Glycol at 87°C, at 1000hrs
 95% Initial Strength RetainedMotor Oil at 125°C, at 1000hrs
 95% Initial Strength RetainedGasoline at 22°C, at 1000hrs
 95% Initial Strength RetainedBrake Fluid at 22°C, at 1000hrs
CompositionMethacrylate ester
Torque>2.8 N.mBreakaway, M10 steel nuts and bolts, ISO 10964
 1 N.mPrevail, M10 steel nuts and bolts, ISO 10964

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPALML059 / 135213

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.