MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Crosspolimeri FRAGOM PR/112 UTW Flame Retardant Polyolefinic
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: FRAGOM: is the trade mark of our flame retardant polyolefinic compounds.

FRAGOM PR/112 UTW: low halogen flame-retardant thermoplastic compound suitable for UTW automotive cables insulation. Exercise temperature: - 40 +125°C

Certify: LV112- ISO 6722 Class C, FIAT 7.Z8220 T3 (Ultra Sottili / Ultra Tin)

Information provided by Crosspolimeri S.P.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.21 g/cc1.21 g/ccASTM D792
Melt Flow 15 g/10 min
@Load 21.6 kg,
Temperature 230 °C
15 g/10 min
@Load 47.6 lb,
Temperature 446 °F
ASTM D1238
Storage Temperature 12.0 °C53.6 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5858ASTM D2240
Tensile Strength >= 19.0 MPa>= 2760 psiIEC 60811
Elongation at Break >= 250 %>= 250 %IEC 60811
Abrasion >= 200>= 200[cycles]
 
Thermal PropertiesMetricEnglishComments
Oxygen Index 27 %27 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Zone 1 160 °C320 °F
Zone 2 175 °C347 °F
Zone 3 190 °C374 °F
Zone 4 200 °C392 °F
Die Temperature 225 °C437 °F
Head Temperature 210 °C410 °F
Dry Time  2.00 hour
@Temperature 100 °C
2.00 hour
@Temperature 212 °F
 3.00 hour
@Temperature 120 °C
3.00 hour
@Temperature 248 °F
 
Descriptive Properties
Exercise temperature-40 - 125°C
Halogen Content<11%IEC 60754-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCROS088 / 294172

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.