MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M Scotch-Weld™ 2290 Epoxy Adhesive/Coating
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: 3M™ Scotch-Weld™ Epoxy Adhesive/Coating 2290 is an amber tinted thermo-setting adhesive/coating for metal to metal bonding and coating. It can be used to assemble laminated steel cores for electrical motor stator and rotors, to adhere copper foil to B-staged epoxy in the manufacture of printed circuits, and to coat, protect, and utilize coils and electronic subassemblies.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 19.5 - 23 %
Viscosity 40 - 80 cP
 
Mechanical PropertiesOriginal ValueComments
Shear Strength 5000 psiOverlap, Tap Water 30 days @ RT; ASTM D1002-72
 5000 psiOverlap, 20% Salt Spray 30 days @ 35°C; ASTM D1002-72
 5000 psiOverlap, 7 days at RT; ASTM D1002-72
 5000 psiOverlap, Aromatic Fuels 7 days @ RT; ASTM D1002-72
 300 psi
@Temperature 150 °C
Overlap; ASTM D1002
 1200 psi
@Temperature 120 °C
Overlap; ASTM D1002
 3500 psi
@Temperature 82.0 °C
Overlap; ASTM D1002
 5000 psi
@Temperature -55.0 °C
Overlap; ASTM D1002
 5000 psi
@Temperature 24.0 °C
Overlap; ASTM D1002
Peel Strength 10.0 pliT-Peel; ASTM D1876
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.20e+15 ohm-cm
Dielectric Constant 5.2
@Frequency 1000 Hz
Dielectric Strength 2400 kV/in
Dissipation Factor 0.011
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 262 µm/m-°C
@Temperature -20.0 - 70.0 °C
 543 µm/m-°C
@Temperature 100 - 120 °C
Glass Transition Temp, Tg 95.0 °C
Flash Point -14.0 °C
 
Descriptive Properties
AppearanceLight Amber

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Epoxy Adhesive
Overview of materials for Epoxy Cure Resin
Lord Adhesives Thermoset™ EP-809 Ignition Coil Impregnating and Encapsulation Epoxy
Epoxy Technology EPO-TEK® 377 High Temperature Epoxy
3M Scotch-Weld™ 2290 Amber One-Part Epoxy Adhesive

PMM34638 / 169385

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.