MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

DuPont Mobility and Materials Delrin® DE10010 ® NC000 Stainless Steel Filled Acetal  (discontinued **)
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: DE10010 is a development grade with moderate surface conductivity, designed to add static dissipation of electric charge. It has high elongation, toughness, and good fuel resistance.

Information provided by DuPont

Information provided by DuPont; The Delrin product line was sold by DuPont in 2023 but this specific grade was discontinued prior to the sale

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.46 g/cc0.0527 lb/in³ISO 1183
Linear Mold Shrinkage 0.020 cm/cm0.020 in/in4 mm; ISO 294-4
Linear Mold Shrinkage, Transverse 0.015 cm/cm0.015 in/in4 mm; ISO 294-4
Melt Flow 3.0 g/10 min3.0 g/10 min190°C, 2.16 kg; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 58.0 MPa8410 psiISO 527-1/-2
Elongation at Break 17 %17 %Nominal; ISO 527-1/-2
Elongation at Yield 9.0 %9.0 %ISO 527-1/-2
Tensile Modulus 2.80 GPa406 ksiISO 527-1/-2
Flexural Modulus 2.60 GPa377 ksiISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²2.38 ft-lb/in²ISO 180/1A
Charpy Impact, Notched 0.400 J/cm²1.90 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.00e+7 ohm-cm3.00e+7 ohm-cmIEC 60093
Surface Resistivity per Square 90000 ohm90000 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
Melting Point 166 °C331 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 145 °C293 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 83.0 °C181 °FISO 75-1/-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 190 - 210 °C374 - 410 °F
Mold Temperature 80.0 - 100 °C176 - 212 °F
Moisture Content <= 0.050 %<= 0.050 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDTAL029 / 32349

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.