MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Cast Stainless Steel CA15MA
Categories: Metal; Ferrous Metal; Stainless Steel; Cast Stainless Steel

Material Notes: Martensitic, Normalized, Tempered

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 620 - 795 MPa89900 - 115000 psi
Tensile Strength, Yield >= 450 MPa>= 65300 psi
Elongation at Break >= 18 %>= 18 %
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.15 %<= 0.15 %
Chromium, Cr 11.5 - 14 %11.5 - 14 %
Copper, Cu >= 0.50 %>= 0.50 %
Iron, Fe 82 - 87.9 %82 - 87.9 %As remainder
Manganese, Mn <= 1.0 %<= 1.0 %
Molybdenum, Mo 0.15 - 1.0 %0.15 - 1.0 %
Nickel, Ni <= 1.0 %<= 1.0 %
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si <= 0.65 %<= 0.65 %
Sulfur, S <= 0.040 %<= 0.040 %
Tungsten, W <= 0.10 %<= 0.10 %
Vanadium, V <= 0.050 %<= 0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Assab Steels ASSAB XW-42 Cold Work Steel
Latrobe LSS™ H11 Hot Work Tool Steel (ASTM H11)
MetalTek MTEK A2 Cast UNS T90102 Tool Steel
Latrobe LSS™ MGR™ Tool Steel (ASTM A8)
Cast Stainless Steel UNS J91261

MQCCA15B50 / 13332

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.