MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Covestro Makrolon® Rx2430 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: MVR (300 °C/1.2 kg) 19 cm³/10 min; medical devices; suitable for sterilization with high-energy radiation; biocompatible according to many ISO 10993-1 test requirements; low viscosity; injection molding - melt temperature 280 - 320 °C; transparent parts for medical devices

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.660 g/ccpellets; ISO 60
Density 1.20 g/ccISO 1183
Moisture Absorption at Equilibrium 0.12 %ISO 62
Water Absorption at Saturation 0.30 %ISO 62
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cmparallel/normal; b.o. ISO 2577
Linear Mold Shrinkage, Flow 0.0060 cm/cm60x60x2 mm; 500 bar; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0065 cm/cm60x60x2 mm; 500 bar; ISO 294-4
Melt Flow 20 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 118 MPaISO 2039-1
Tensile Strength at Break 75.0 MPa50 mm/min; ISO 527-1/-2
Tensile Strength, Yield 67.0 MPa50 mm/min; ISO 527-1/-2
Elongation at Break >= 50 %Nominal, 50 mm/min; ISO 527-1/-2
 130 %50 mm/min; ISO 527-1/-2
Elongation at Yield 6.1 %50 mm/min; ISO 527-1/-2
Tensile Modulus 2400 MPa1 mm/min; ISO 527-1/-2
Flexural Strength 100 MPa2 mm/min; ISO 178
Flexural Yield Strength 74.0 MPa
@Strain 3.5 %
2 mm/min; ISO 178
Flexural Modulus 2.40 GPa2 mm/min; ISO 178
Flexural Strain at Yield 7.0 %2 mm/min; ISO 178
Izod Impact, Notched (ISO) 12.0 kJ/m²
@Thickness 3.00 mm,
Temperature -30.0 °C
complete break; ISO 7391/b.o. ISO 180-A
 60.0 kJ/m²
@Thickness 3.00 mm,
Temperature 23.0 °C
partial break; ISO 7391/b.o. ISO 180-A
Charpy Impact Unnotched NBISO 179/1eU
 NB
@Temperature -30.0 °C
ISO 179/1eU
 NB
@Temperature -60.0 °C
ISO 179/1eU
Charpy Impact, Notched 1.40 J/cm²
@Thickness 3.00 mm,
Temperature -30.0 °C
complete break; ISO 7391/b.o. ISO 179-1eA
 7.00 J/cm²
@Thickness 3.00 mm,
Temperature 23.0 °C
partial break; ISO 7391/b.o. ISO 179-1eA
Impact 5300Puncture - maximum force (N); ISO 6603-2
 6200
@Temperature -30.0 °C
Puncture - maximum force (N); ISO 6603-2
Puncture Energy 60.0 JISO 6603-2
 70.0 J
@Temperature -30.0 °C
ISO 6603-2
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+16 ohmIEC 60093
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 65.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
CTE, linear, Transverse to Flow 65.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
Thermal Conductivity 0.200 W/m-Kcross-flow; ISO 8302
Hot Ball Pressure Test 132 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 134 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 122 °CISO 75-1/-2
Vicat Softening Point 141 °C50°C/h 50N; ISO 306
 142 °C120°C/h 50N; ISO 306
Flammability, UL94 V-2
@Thickness 0.360 mm
Flash Point 480 °Cignition; ASTM D1929
 550 °Cself ignition; ASTM D1929
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 °CInjection Molding; ISO 294
Mold Temperature 80.0 °CInjection Molding; ISO 294
Injection Velocity 200 mm/secISO 294

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Makrolon® Rx2530 Polycarbonate
Plaskolite West Optix® CA-1000 I Clear High Impact Acrylic Resin
Celanese Celcon® MT8U01 Medical Grade Acetal Copolymer
Covestro Makrolon® 2258 Polycarbonate
Covestro Makrolon® 2408 Polycarbonate

PB09969 / 92809

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.