MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Morgan Advanced Ceramics Superwool® VF Shapes and Boards HT 2 VF Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Superwool ® HT 2™ VF offers record performances compared to the original formula because of its resistance to higher temperature, while maintaining a low thermal conductivity and good resistance to erosion. Use in conditions with repeated shocks must be avoided.

Typical applications:

  • Riser sleeves and crucibles for ferrous and non ferrous molten metals
  • Stopper nut insulation
  • Ladle shroud gasket
  • Nozzle insulation in continuous casting
  • Roller inserts in roller hearth furnace
  • Glass casting mould
  • Tube insulation end in tube fumes boiler
  • Insulation for domestic appliance
  • Furnace insulation

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.335 g/cc0.0121 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.00187 GPa0.271 ksiunfired
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.0800 W/m-K
@Temperature 400 °C
0.555 BTU-in/hr-ft²-°F
@Temperature 752 °F
ASTM C-201
 0.120 W/m-K
@Temperature 600 °C
0.833 BTU-in/hr-ft²-°F
@Temperature 1110 °F
ASTM C-201
 0.180 W/m-K
@Temperature 800 °C
1.25 BTU-in/hr-ft²-°F
@Temperature 1470 °F
ASTM C-201
 0.250 W/m-K
@Temperature 1000 °C
1.74 BTU-in/hr-ft²-°F
@Temperature 1830 °F
ASTM C-201
 0.330 W/m-K
@Temperature 1200 °C
2.29 BTU-in/hr-ft²-°F
@Temperature 2190 °F
ASTM C-201
 0.380 W/m-K
@Temperature 1300 °C
2.64 BTU-in/hr-ft²-°F
@Temperature 2370 °F
ASTM C-201
Shrinkage <= 2.0 %
@Temperature 1400 °C,
Time 86400 sec
<= 2.0 %
@Temperature 2550 °F,
Time 24.0 hour
isothermal, permanent
 
Component Elements PropertiesMetricEnglishComments
Loss on Ignition(%) 4.0 %4.0 %
 
Descriptive Properties
Classification Temperature (°C)1450
Colorwhite/tan

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CMORF7020 / 203319

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.