Daplen FS65T20 is a 20% mineral filled polypropylene compound intended for injection molding. FS65T20 has been developed especially for applications requiring high detergent resistance and heat stability. FS65T20 has well balanced mechanical properties, medium flow rate and good processability and its tested and approved according to UL94 HB. Daplen FS65T20 has been developed for washing machine parts, dishwasher components, and household appliances. Information provided by the Manufacturer. |