Temper: Hard Fabrication Properties: Excellent Suitability – Soldering, Capacity for Being Cold Worked; Good Suitability – Brazing; Fair Suitability – Oxyacetylene Welding, Gas Shielded Arc Welding, Spot Weld, Butt Weld; Poor Suitability – Capacity for Being Hot Formed Common Fabrication Processes: Forming and Bending; Machining; Piercing and Punching Typical uses: Hydraulic Controls; Power and Pump Cylinder Liners; Power and Pump Cylinders; Screw Machine Products; Primers; Plumbing Accessories; Plumbing Brass Goods Applicable Specifications: Seamless Tube – ASME SB135; Tube – AMS 4558, MILITARY MIL-T-46072, Seamless (Metric) ASTM B135/B135M, ASTM B135 |