MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
IRPC Polimaxx Pentfoam 193L Expandable Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: General: Pentfoam 139L is a regular grade expandable polystyrene containing pentane as blowing agent. This grade is developed to meet the demand for fast molding cycles in vacuum machine.

Applications: Pentfoam 193L is particularly well suited for hte manufacture of eps low density insulation boards from block molding. This grade is always widely used for the production of low density decoration products, and drainage boards.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0120 - 0.0130 g/cc
 0.0120 - 0.0200 g/ccmolding density range
Bead Size 1.25 - 2.50 mm
Maximum Moisture Content 0.20
 
Chemical PropertiesOriginal ValueComments
Blowing Agent Content >= 6.0 %
 
Mechanical PropertiesOriginal ValueComments
K Factor (Wear Factor) 56 - 58

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Jackon JACKOCELL® R311 Expanded Polystyrene Packaging and Shape Molding
LG Chemical R160 EPS, Flame Retardant
NOVA Chemicals Arcel 730 70% PS/30% PE Interpolymer
LG Chemical R320 EPS, Flame Retardant
Sekisui PIOCELAN SP-50D Moldable Polymer Foam

PIRPC016 / 83993

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.