The RT500F has good electrical properties under humid conditions, excellent heat resistance and mechanical properties. RT500F is made with a fine weave woven glass fabric, for better machining and a smoother surface finish. It also complies with MIL-I-24768/2, Type GEE and ASTM D709 Type IV Grade G-10.Information provided by Norplex-Micarta |
Fiber Glass, Epoxy, Micarta, NEMA G-10, MIL-I-24768/2 Type GEE, ASTM D709 Type IV Grade G-10 |