MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company Permaprene™ 2800 B-75A Z Thermoplastic Polyolefin Elastomer (TEO), FDA Compliant Ingredients
Categories: Polymer; Thermoplastic; Elastomer, TPE

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.01 g/cc1.01 g/ccASTM D 792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 808010 s delay; ASTM D 2240
Tensile Strength at Break  3.45 MPa
@Thickness 3.20 mm
500 psi
@Thickness 0.126 in
Die C; 20 in/min (500 mm/min); ASTM D 638
 7.58 MPa
@Thickness 3.20 mm
1100 psi
@Thickness 0.126 in
Die C, 20 in/min (500 mm/min); ASTM D 412
100% Modulus 3.79 MPa
@Strain 100 %,
Thickness 3.20 mm
550 psi
@Strain 100 %,
Thickness 0.126 in
Die C; 20 in/min (500 mm/min); ASTM D 412
Tear Strength 35.1 kN/m200 pliDie C; ASTM D 624
Compression Set  30 %
@Temperature 23.0 °C,
Time 79200 sec
30 %
@Temperature 73.4 °F,
Time 22.0 hour
Method B; Type 2; ASTM D 395
 48 %
@Temperature 70.0 °C,
Time 79200 sec
48 %
@Temperature 158 °F,
Time 22.0 hour
Method B; Type 2; ASTM D 395
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 193 - 227 °C380 - 440 °F
Mold Temperature 10.0 - 79.4 °C50.0 - 175 °F
Drying Temperature 79.4 °C
@Time 7200 - 10800 sec
175 °F
@Time 2.00 - 3.00 hour
Moisture Content <= 0.080 %<= 0.080 %
Dew Point -17.8 °C0.000 °F
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PQZWA10733 / 90539

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.