MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Stratasys® Ultem 9085 for Rapid Prototyping
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: ULTEM™ 9085 resin filament is a PEI (polyetherimide) thermoplastic FDM material. It features a high strength-to-weight ratio, high thermal and chemical resistance, and meets multiple aerospace and railway industry standards for flame, smoke and toxicity (FST) characteristics. ULTEM™ 9085 resin CG (Certified Grade) meets more stringent test criteria and possesses documented traceability from filament back to raw material lot number. Included documentation:
  • Certificate of Analysis – for both raw material and filament are supplied, documenting test results and identification to match filament manufacturing lot number to raw material batch number.
  • Certificate of Conformance – confirms that the material is manufactured in compliance to approved Stratasys and industry specifications.
Typical applications include production parts and functional prototypes. Available colors are natural and black.

Information provided by Stratasys.

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.27 g/ccXY, XZ/ZX Orientations; ASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 40.0 MPaZX Orientation, Black T16 tip; ASTM D638
 40.0 MPaZX Orientation, T20 tip; ASTM D638
 49.0 MPaZX Orientation, T16 tip; ASTM D638
 68.0 MPaXZ Orientation, T16 tip; ASTM D638
 68.0 MPaXZ Orientation, T20 tip; ASTM D638
 70.0 MPaXZ Orientation, Black T16 tip; ASTM D638
Tensile Strength, Ultimate 58.0 MPaZX Orientation, T16A tip; ASTM D638
 77.0 MPaXZ Orientation, T16A tip; ASTM D638
Tensile Strength, Yield 68.0 MPaXZ Orientation, T20 tip; ASTM D638
 70.0 MPaXZ Orientation, Black T16 tip; ASTM D638
 70.0 MPaXZ Orientation, T16 tip; ASTM D638
 38.0 MPa
@Strain 0.2 %
ZX Orientation, T16A tip; ASTM D638
 45.0 MPa
@Strain 0.2 %
XZ Orientation, T16A tip; ASTM D638
Elongation at Break 1.9 %ZX Orientation, T16 tip; ASTM D638
 2.1 %ZX Orientation, Black T16 tip; ASTM D638
 2.5 %ZX Orientation, T20 tip; ASTM D638
 5.4 %XZ Orientation, Black T16 tip; ASTM D638
 5.4 %XZ Orientation, T16 tip; ASTM D638
 5.7 %XZ Orientation, T20 tip; ASTM D638
Elongation at Yield 5.3 %XZ Orientation, T16 tip; ASTM D638
 5.5 %XZ Orientation, Black T16 tip; ASTM D638
 5.8 %XZ Orientation, T20 tip; ASTM D638
Modulus of Elasticity 1.98 GPaZX Orientation, T20 tip; ASTM D638
 2.31 GPaXZ Orientation, T20 tip; ASTM D638
 2.41 GPaZX Orientation, Black T16 tip; ASTM D638
 2.41 GPaZX Orientation, T16 tip; ASTM D638
 2.41 GPaZX Orientation, T16A tip; ASTM D638
 2.51 GPaXZ Orientation, T16 tip; ASTM D638
 2.53 GPaXZ Orientation, Black T16 tip; ASTM D638
 2.61 GPaXZ Orientation, T16A tip; ASTM D638
Flexural Strength 60.0 MPaZX Orientation, T16 tip; ASTM D790, Procedure A
 60.0 MPaZX Orientation, T20 tip; ASTM D790, Procedure A
 70.0 MPaZX Orientation, Black T16 tip; ASTM D638
 90.0 MPaUltimate, ZX Orientation, T16A tip; ASTM D790, Procedure A
 130 MPaUltimate, XZ Orientation, T16A tip; ASTM D790, Procedure A
 100 MPa
@Strain 5.0 %
XZ Orientation, T16 tip; ASTM D790, Procedure A
 100 MPa
@Strain 5.0 %
XZ Orientation, T20 tip; ASTM D790, Procedure A
 105 MPa
@Strain 5.0 %
XZ Orientation, Black T16 tip; ASTM D638
Flexural Modulus 1.93 GPaZX Orientation, T20 tip; ASTM D790, Procedure A
 2.10 GPaZX Orientation, Black T16 tip; ASTM D790, Procedure A
 2.12 GPaZX Orientation, T16 tip; ASTM D790, Procedure A
 2.38 GPaXZ Orientation, T20 tip; ASTM D790, Procedure A
 2.40 GPaXZ Orientation, T16 tip; ASTM D790, Procedure A
 2.47 GPaXZ Orientation, Black T16 tip; ASTM D790, Procedure A
 2.62 GPaXZ Orientation, T16A tip; ASTM D790, Procedure A
 2.96 GPaZX Orientation, T16A tip; ASTM D790, Procedure A
Flexural Strain at Break 3.2 %ZX Orientation, T20 tip; ASTM D790, Procedure A
 3.7 %ZX Orientation, T16 tip; ASTM D790, Procedure A
 3.8 %ZX Orientation, Black T16 tip; ASTM D790, Procedure A
Compressive Yield Strength 85.0 MPaXZ Orientation, T20 tip; ASTM D695
 140 MPaXZ Orientation, Black T16 tip; ASTM D695
 140 MPaXZ Orientation, T16 tip; ASTM D695
 210 MPaZX Orientation, T20 tip; ASTM D695
 340 MPaZX Orientation, T16 tip; ASTM D695
 350 MPaZX Orientation, Black T16 tip; ASTM D695
 63.0 MPa
@Strain 0.2 %
XZ Orientation, T16A tip; ASTM D695
 78.0 MPa
@Strain 0.2 %
ZX Orientation, T16A tip; ASTM D695
Compressive Modulus 1.55 GPaXZ Orientation, T20 tip; ASTM D695
 2.21 GPaXZ Orientation, T16 tip; ASTM D695
 2.27 GPaXZ Orientation, Black T16 tip; ASTM D695
 2.28 GPaZX Orientation, T16 tip; ASTM D695
 2.28 GPaZX Orientation, T20 tip; ASTM D695
 2.36 GPaZX Orientation, Black T16 tip; ASTM D695
 2.62 GPaXZ Orientation, T16A tip; ASTM D695
 2.96 GPaZX Orientation, T16A tip; ASTM D695
Izod Impact, Notched 2.98 J/mZX Orientation, T20 tip; ASTM D256, ASTM D4812
 10.0 J/mXZ Orientation, T20 tip; ASTM D256, ASTM D4812
 37.0 J/mZX Orientation, Black T16 tip; ASTM D256, ASTM D4812
 40.0 J/mZX Orientation, T16 tip; ASTM D256, ASTM D4812
 69.3 J/mZX Orientation, T16A tip; ASTM D256, ASTM D4812
 73.7 J/mXZ Orientation, T16A tip; ASTM D256, ASTM D4812
 88.0 J/mXZ Orientation, T16 tip; ASTM D256, ASTM D4812
 95.0 J/mXZ Orientation, Black T16 tip; ASTM D256, ASTM D4812
Izod Impact, Unnotched 12.0 J/mZX Orientation, T20 tip; ASTM D256, ASTM D4812
 80.0 J/mXZ Orientation, T20 tip; ASTM D256, ASTM D4812
 168 J/mZX Orientation, Black T16 tip; ASTM D256, ASTM D4812
 187 J/mZX Orientation, T16 tip; ASTM D256, ASTM D4812
 650 J/mXZ Orientation, T16 tip; ASTM D256, ASTM D4812
 770 J/mXZ Orientation, Black T16 tip; ASTM D256, ASTM D4812
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 6.89e+15 ohm-cmXY, XZ/ZX Orientations; ASTM D257
Dielectric Constant 2.7
@Frequency 1000 Hz
XY, XZ/ZX Orientations; ASTM D150
 2.8
@Frequency 2.00e+6 Hz
XY, XZ/ZX Orientations; ASTM D150
Dissipation Factor 0.0020
@Frequency 1000 Hz
XY, XZ/ZX Orientations; ASTM D150
 0.010
@Frequency 2.00e+6 Hz
XY, XZ/ZX Orientations; ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 32.0 µm/m-°C
@Temperature 80.0 - 160 °C
XY, XZ/ZX Orientations; ASTM E831
 45.0 µm/m-°C
@Temperature -50.0 - 80.0 °C
XY, XZ/ZX Orientations; ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 177 °CXY, XZ/ZX Orientations; ASTM D648 Method B
Deflection Temperature at 1.8 MPa (264 psi) 173 °CXY, XZ/ZX Orientations; ASTM D648 Method B
Glass Transition Temp, Tg 180 °CInflection Point, XY, XZ/ZX; ASTM D7426
Flammability, UL94 V-0ANSI/UL 746B, Blue Card #E345258
 
Descriptive Properties
FAA Flammability<5FAR 25.853, method A/B
OSU Peak Heat Release36 kW/m2FAR25.853, 5 min test
OSU Total Heat Release16 kW-min/m2FAR25.853, 2 min test
Vertical Burnpasses at 2 secondsTest at 60s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Proto3000 ULTEM* 9085 Fused Deposition Modeling Polymer
Stratasys® PC Polycarbonate for 3D Printing
Stratasys® PPSF Polyphenylsulfone for 3D Printing
Stratasys® PC-ABS
Stratasys® ABS-M30

PSTRAT016 / 89256

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.