MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Low Density Polyethylene (LDPE), Extrusion Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Extrusion Grade

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Extrusion Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.915 - 0.960 g/ccAverage value: 0.921 g/cc Grade Count:134
Moisture Vapor Transmission 0.410 - 0.410 cc-mm/m²-24hr-atm
@Temperature 37.8 - 37.8 °C
Average value: 0.410 cc-mm/m²-24hr-atm Grade Count:1
 0.410 - 0.410 cc-mm/m²-24hr-atm
@Thickness 0.0254 - 0.0254 mm
Average value: 0.410 cc-mm/m²-24hr-atm Grade Count:1
Water Vapor Transmission 0.260 - 27.9 g/m²/dayAverage value: 14.2 g/m²/day Grade Count:12
 17.0 - 18.0 g/m²/day
@Temperature 37.8 - 38.0 °C
Average value: 17.9 g/m²/day Grade Count:4
 18.0 - 18.5 g/m²/day
@Temperature 37.8 - 37.8 °C
Average value: 17.9 g/m²/day Grade Count:2
 18.0 - 18.5 g/m²/day
@Thickness 0.0250 - 0.0250 mm
Average value: 17.9 g/m²/day Grade Count:2
Oxygen Transmission Rate 6670 - 7600 cc/m²/dayAverage value: 7290 cc/m²/day Grade Count:4
Environmental Stress Crack Resistance 18.0 - 10000 hourAverage value: 2550 hour Grade Count:4
Oxidative Induction Time (OIT) >= 40.0 min
@Temperature 200 - 200 °C
Average value: 40.0 min Grade Count:1
Thickness 25.0 - 150 micronsAverage value: 54.3 microns Grade Count:24
Melt Flow 0.160 - 55.0 g/10 minAverage value: 5.48 g/10 min Grade Count:120
Base Resin Melt Index 0.330 - 7.00 g/10 minAverage value: 2.98 g/10 min Grade Count:14
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 42.0 - 56.0Average value: 48.4 Grade Count:28
Tensile Strength, Ultimate 8.96 - 54.0 MPaAverage value: 12.6 MPa Grade Count:42
Film Tensile Strength at Yield, MD 10.0 - 15.2 MPaAverage value: 12.3 MPa Grade Count:15
Film Tensile Strength at Yield, TD 9.00 - 15.2 MPaAverage value: 11.4 MPa Grade Count:15
Tensile Strength, Yield 7.60 - 14.0 MPaAverage value: 10.1 MPa Grade Count:25
Film Elongation at Break, MD 150 - 580 %Average value: 321 % Grade Count:60
Film Elongation at Break, TD 220 - 1110 %Average value: 621 % Grade Count:60
Elongation at Break 164 - 920 %Average value: 518 % Grade Count:43
Modulus of Elasticity 0.152 - 0.290 GPaAverage value: 0.207 GPa Grade Count:11
Flexural Modulus 0.0700 - 0.448 GPaAverage value: 0.199 GPa Grade Count:27
Secant Modulus 0.166 - 0.372 GPaAverage value: 0.238 GPa Grade Count:11
Secant Modulus, MD 0.0830 - 1.28 GPaAverage value: 0.216 GPa Grade Count:24
Secant Modulus, TD 0.124 - 1.18 GPaAverage value: 0.239 GPa Grade Count:24
Coefficient of Friction 0.450 - 0.600Average value: 0.550 Grade Count:3
Elmendorf Tear Strength MD 100 - 600 gAverage value: 348 g Grade Count:31
Elmendorf Tear Strength TD 55.0 - 500 gAverage value: 217 g Grade Count:41
Elmendorf Tear Strength, MD 2.50 - 12.0 g/micronAverage value: 8.19 g/micron Grade Count:21
Elmendorf Tear Strength, TD 2.20 - 7.00 g/micronAverage value: 4.71 g/micron Grade Count:22
Dart Drop 2.00 - 11.0 g/micronAverage value: 3.48 g/micron Grade Count:24
Dart Drop Test 25.0 - 650 gAverage value: 142 g Grade Count:42
Hot Tack Strength 225 g/25 mmAverage value: 225 g/25 mm Grade Count:3
 225 - 225 g/25 mm
@Temperature 38.0 - 38.0 °C
Average value: 225 g/25 mm Grade Count:1
Film Tensile Strength at Break, MD 11.0 - 78.5 MPaAverage value: 25.4 MPa Grade Count:60
Film Tensile Strength at Break, TD 10.0 - 53.9 MPaAverage value: 19.7 MPa Grade Count:60
Heat Seal Strength 1400 g/25 mmAverage value: 1400 g/25 mm Grade Count:3
 1400 - 1400 g/25 mm
@Temperature 38.0 - 38.0 °C
Average value: 1400 g/25 mm Grade Count:1
Heat Seal Strength Initiation Temperature 105 °CAverage value: 105 °C Grade Count:3
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.27 - 2.29Average value: 2.28 Grade Count:3
Dissipation Factor 0.0000400 - 0.000100Average value: 0.0000640 Grade Count:3
 
Thermal PropertiesOriginal ValueComments
Melting Point 102 - 113 °CAverage value: 108 °C Grade Count:41
Vicat Softening Point 84.0 - 128 °CAverage value: 91.0 °C Grade Count:75
Brittleness Temperature -76.0 - -60.0 °CAverage value: -73.5 °C Grade Count:8
 
Optical PropertiesOriginal ValueComments
Haze 1.10 - 19.0 %Average value: 8.09 % Grade Count:48
Gloss 10.0 - 112 %Average value: 70.6 % Grade Count:42
 
Processing PropertiesOriginal ValueComments
Processing Temperature 145 - 340 °CAverage value: 208 °C Grade Count:9
Adapter Temperature 204 - 218 °CAverage value: 211 °C Grade Count:3
Die Temperature 150 - 220 °CAverage value: 187 °C Grade Count:8
Melt Temperature 110 - 364 °CAverage value: 222 °C Grade Count:70

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Low Density Polyethylene (LDPE), Molded
Overview of materials for High Density Polyethylene (HDPE), Extruded
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
Overview of materials for Low Density Polyethylene (LDPE), Film Grade
Overview of materials for Polypropylene, Extrusion Grade

O3801 / 78248

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.