MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Copper Alloy, UNS C40950, H02 Temper, Strip
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: 1/2 Hard

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Capacity for Being Cold Worked, Capacity for Being Hot Formed; Good Suitability –Gas Shielded Arc Welding, Butt Weld; Fair Suitability – Oxyacetylene Welding, Coated Metal Arc Welding, Spot Weld, Seam Weld

Typical Uses: Connectors, automotive; Electric & Electronic parts

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.320 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 160
@Load 3.00 kg
Tensile Strength 73.0 ksiTypical
 67.0 - 80.0 ksi
Tensile Strength, Yield 70.0 ksi0.2% Offset, Typical
 64.0 - 77.0 ksi0.2% Offset
Elongation at Break 8.0 %
Tensile Modulus 17400 ksi
Modulus of Rigidity 6500 ksi
Poissons Ratio 0.34Calculated
Machinability 30 %
Forgeability 60 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000610 ohm-cm28% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.0 µin/in-°F
@Temperature 20.0 - 100 °C
 10.0 µin/in-°F
@Temperature 20.0 - 200 °C
 10.0 µin/in-°F
@Temperature 20.0 - 300 °C
Thermal Conductivity 98.0 BTU-in/hr-ft²-°F
Melting Point 1904 - 1940 °F
Solidus 1904 °F
Liquidus 1940 °F
Annealing Point >= 930 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature 570 °FStress Relief
Hot-Working Temperature >= 1560 °F
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 91.5 - 94.5 %
Iron, Fe <= 0.030 %
Lead, Pb <= 0.050 %
Nickel, Ni 0.30 - 0.80 %
Phosphorus, P 0.010 - 0.080 %
Tin, Sn 0.30 - 0.80 %
Zinc, Zn 3.8 - 7.9 %As Balance
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC40950x1 / 291900

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.