MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

A. Schulman BMC T60-6009 Compression Grade Wear Resistant Molding Compound
Categories: Polymer; Thermoset; Polyester, TS; Polyester (Thermoset) - Rigid

Material Notes: BMC T60-6009 is a compression grade wear resistant molding compound. This material was specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cost per cubic inch savings. BMC T60-6009 is UL listed and is typically used in power distribution equipment, switching components/relays, constant use switch applications and circuit protection breakers.

Information provided by Bulk Molding Compounds, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.52 - 1.72 g/cc0.0549 - 0.0621 lb/in³Molded
Linear Mold Shrinkage 0.0030 - 0.0040 cm/cm0.0030 - 0.0040 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 5.0 - 105.0 - 10
Tensile Strength 31.0 - 44.8 MPa4500 - 6500 psi
Flexural Strength 58.6 - 86.2 MPa8500 - 12500 psi
Flexural Modulus 3.79 - 5.17 GPa550 - 750 ksi
Compressive Strength 95.1 - 123 MPa13800 - 17800 psi
Izod Impact, Notched 1.60 - 2.67 J/cm3.00 - 5.00 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 13.2 - 15.2 kV/mm335 - 385 kV/inshort time
Arc Resistance >= 190 sec>= 190 sec
Comparative Tracking Index >= 500 V>= 500 V
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C>= 500 °F
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Processing Temperature 138 - 166 °C280 - 330 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman BMC A50-XHS High Strength Grade Molding Compound
A. Schulman BMC Super-Tough Mineral Filled, Glass Reinforced Polyester
A. Schulman BMC T40-4020-AQ High Strength Arc Quenching Molding Compound
A. Schulman BMC T44 High Strength Mineral Filled Molding Compound
A. Schulman BMC G10(12) Mineral Filled, Glass Fiber Reinforced Polyester

PBMC945 / 123409

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.