MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SABIC ULTEM™ Resin 2210F Polyetherimide (PEI) (Europe)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors.

Features: High Stiffness,Hydrolytic Stability,Chemical Resistance,Easy Flow,Low Smoke and Toxicity,Good Mechanicals in Broad Temperature Range,Low Creep Sensitivity,Low Shrinkage,Good metal adhesion,Amorphous,High Strength,General Purpose,High Heat Resistance,Good dimensional stability,Flame Retardant,Food Contact Acceptable

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.42 g/cc0.0513 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.550 %0.550 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 1.0 %1.0 %ISO 62-1
Viscosity 10 cP
@Load 5.00 kg,
Temperature 360 °C
10 cP
@Load 11.0 lb,
Temperature 680 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm0.0030 - 0.0050 in/inSABIC method
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 150 MPa21800 psiH358/30; ISO 2039-1
Tensile Strength at Break 140 MPa20300 psi5 mm/min; ISO 527
Elongation at Break 2.0 %2.0 %5 mm/min; ISO 527
Tensile Modulus 6.80 GPa986 ksi1 mm/min; ISO 527
Flexural Strength 210 MPa30500 psibreak, 2mm/min; ISO 178
Flexural Modulus 6.50 GPa943 ksi2 mm/min; ISO 178
Izod Impact, Unnotched (ISO) 30.0 kJ/m²14.3 ft-lb/in²80*10*4; ISO 180/1U
 30.0 kJ/m²
@Temperature -30.0 °C
14.3 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1U
Charpy Impact Unnotched 3.50 J/cm²16.7 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eU
 3.50 J/cm²
@Temperature -30.0 °C
16.7 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 0.900 J/cm²4.28 ft-lb/in²ISO 179/2C
Taber Abrasion, mg/1000 Cycles 1717CS-17, 1 kg; SABIC method
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmROA; IEC 60093
Dielectric Constant  3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
IEC 60250
 3.1
@Frequency 50.0 - 60.0 Hz
3.1
@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength  16.0 kV/mm
@Thickness 3.20 mm
406 kV/in
@Thickness 0.126 in
in oil; IEC 60243-1
 26.0 kV/mm
@Thickness 1.60 mm
660 kV/in
@Thickness 0.0630 in
in oil; IEC 60243-1
 34.0 kV/mm
@Thickness 0.800 mm
864 kV/in
@Thickness 0.0315 in
in oil; IEC 60243-1
Dissipation Factor  0.00080
@Frequency 50.0 - 60.0 Hz
0.00080
@Frequency 50.0 - 60.0 Hz
IEC 60250
 0.0025
@Frequency 1e+6 Hz
0.0025
@Frequency 1e+6 Hz
IEC 60250
 0.0049
@Frequency 2.45e+9 Hz
0.0049
@Frequency 2.45e+9 Hz
IEC 60250
Arc Resistance 60 - 120 sec60 - 120 secASTM D495
Comparative Tracking Index 100 V100 VIEC 60112
 100 - 175 V100 - 175 VUL 746A
 150 V150 VIEC 60112
Hot Wire Ignition, HWI  30 - 60 sec
@Thickness >=1.50 mm
30 - 60 sec
@Thickness >=0.0591 in
UL 746A
 60 - 120 sec
@Thickness >=3.00 mm
60 - 120 sec
@Thickness >=0.118 in
UL 746A
High Amp Arc Ignition, HAI  0.00 - 15 arcs
@Thickness >=3.00 mm
0.00 - 15 arcs
@Thickness >=0.118 in
UL 746A
 15 - 30 arcs
@Thickness >=1.50 mm
15 - 30 arcs
@Thickness >=0.0591 in
UL 746A
High Voltage Arc-Tracking Rate, HVTR 25.4 - 80.0 mm/min1.00 - 3.15 in/minUL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 25.0 µm/m-°C
@Temperature 23.0 - 150 °C
13.9 µin/in-°F
@Temperature 73.4 - 302 °F
ISO 11359-2
CTE, linear, Transverse to Flow 60.0 µm/m-°C
@Temperature 23.0 - 150 °C
33.3 µin/in-°F
@Temperature 73.4 - 302 °F
ISO 11359-2
Thermal Conductivity 0.280 W/m-K1.94 BTU-in/hr-ft²-°FISO 8302
Hot Ball Pressure Test 125 °C257 °FPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 210 °C410 °FEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 205 °C401 °FEdgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 212 °C414 °FRate B/50; ISO 306
 218 °C424 °FRate B/120; ISO 306
 223 °C433 °FRate A/50; ISO 306
UL RTI, Electrical 170 °C338 °FUL 746B
UL RTI, Mechanical with Impact 170 °C338 °FUL 746B
UL RTI, Mechanical without Impact 170 °C338 °FUL 746B
Flammability, UL94  V-0
@Thickness >=0.410 mm
V-0
@Thickness >=0.0161 in
UL 94
 5VA
@Thickness >=1.90 mm
5VA
@Thickness >=0.0748 in
UL 94
Oxygen Index 46 %46 %ISO 4589
Glow Wire Flammability Index 960 °C
@Thickness 3.20 mm
1760 °F
@Thickness 0.126 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 360 - 410 °C680 - 770 °F
Zone 2 360 - 410 °C680 - 770 °F
Zone 3 370 - 420 °C698 - 788 °F
Melt Temperature 370 - 410 °C698 - 770 °FInjection Molding
Mold Temperature 140 - 180 °C284 - 356 °F
Drying Temperature 150 °C302 °FInjection Molding
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hourInjection Molding
Precipitation Temperature 80.0 - 120 °C176 - 248 °FHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82608 / 290555

Ensinger SPI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.