MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Aptek 2503R-A/B Premeasured conformal urethane coating repair kit
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes: APTEK 2503-A/B is an unfilled, two component, electrically insulating, transparent, flexible urethane coating system designed for the encapsulation and protection of electrical/electronic components mounted on printed circuit boards.

Ideal for repair-ready-to-use; Fully compatible with APTEK 2503-A/B conformal coating as well as other commercially available urethane coatings; Excellent reversion resistance for good physical stability under high heat and humidity environments; Tg below -70ºC for excellent low temperature cycling, storage and performance; Excellent substrate adhesion, superior to silicones; Exceeds NASA outgassing requirements for high vacuum environments; Fluoresces under black-light (UV) to facilitate QC inspection of coating coverage of repaired components/substrates.

APTEK 2503R-A is an unfilled polyol resin containing solvent and is thus considered a flammable liquid and should be treated with caution. . APTEK 2503R-B is an organic isocyanate and is safe to handle when used properly. .

Information provided by Aptek Laboratories, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Outgassing - Total Mass Loss 0.187 %0.187 %Cured property; at 10E-6 torr; ASTM E595
Collected Volatile Condensable Material 0.0020 %0.0020 %Cured property; at 10E-6 torr; ASTM E595
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8888Cured property; ASTM D2240
Tensile Strength, Ultimate 19.3 MPa2800 psiCured property; ASTM D412
Elongation at Break 525 %525 %Cured property; ASTM D412
 
Thermal PropertiesMetricEnglishComments
CTE, linear 180 µm/m-°C
@Temperature 20.0 °C
100 µin/in-°F
@Temperature 68.0 °F
Cured property; alpha 1; JMTP P200
Glass Transition Temp, Tg -74.0 °C-101 °FCured property; JMTP P200
Flash Point 10.0 °C50.0 °FA Component; ASTM D92
 >= 150 °C>= 302 °FB Component; ASTM D92
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 °C176 °FCure 8 hrs
 100 °C212 °FCure 5 hrs
 125 °C257 °FCure 2 hrs

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAPTEK30 / 24192

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.