Moplen HP450H is a polypropylene homopolymer used for extrusion applications. Moplen HP450H is formulated with a low water-carry-over additive package. Typical applications are strapping, sheets, monofilaments and tapes. Availability: Africa-Middle East; Asia-Pacific; Australia and New Zealand; Europe; South & Central America Application: Raffia/Tapes/Strapping; Strapping Market: Textile Processing Method: Tapes & Raffia Attribute: Homopolymer Information provided by LyondellBasell. |