MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Reynolds Free Form™ Air HT Low density, lightweight epoxy putty
Categories: Polymer; Thermoset; Epoxy

Material Notes: Product Overview: Free Form™ AIR HT is a low density, lightweight epoxy putty that offers high temperature resistance to 300°F/149°C when cured at room temperature and 400°F/204°C when heat post cured. This is a low-odor, low shrinkage formula that is easy to use. Free Form™ AIR HT is mixed by hand with a 2A:1B by volume or weight mix ratio. It offers a long working time and cures overnight at room temperature to a hard, rigid epoxy that is very strong with modeling board-like properties. It can be sanded, shaped, drilled, tapped and CNC machined/routered. Epoxy Laminating; Laminate Free Form™ AIR HT putty in between layers of EpoxAmite™ HT Laminating Epoxy and fiberglass cloth, carbon or other fiber for making lightweight composite parts. Eliminates the need to make multiple layers of laminating with liquid epoxy; saves time and labor. Epoxy Tooling Applications – use as a filleting material. Also good for jig and fixture construction. Used as a lightweight adhesive, Free Form™ AIR HT will bond to itself and a variety of surfaces including wood, stone and EpoxAcoat™ HT surface coat epoxy. Pot Life/Working Time; this material is mass sensitive. The more material you mix at one time, the less time you have to work with it. Working tip; If mixing a large quantity, flatten putty with a rolling pin to reduce mass concentration and extend pot life.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.510 g/cc0.510 g/ccASTM D-1475
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5555ASTM D-2240
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 204 °C399 °FHeat Deflection Temperature; ASTM D-648
 
Processing PropertiesMetricEnglishComments
Cure Time 960 min16.0 hourDemold Time
Pot Life  90.0 min
@Thickness 38.1 mm
90.0 min
@Thickness 1.50 in
ASTM D-2471
 150 min
@Thickness 9.52 mm
150 min
@Thickness 0.375 in
ASTM D-2471
 180 min
@Thickness 3.17 mm
180 min
@Thickness 0.125 in
ASTM D-2471
 
Descriptive Properties
ColorGrey
Mix Ratio2A:1Bby volume
 2A:1Bby weight
Mixed ViscosityDough
Specific Volume54.31[in3/lb]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREYN211 / 296912

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.