MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Overview of materials for Thermoset Polyurethane, Adhesive
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Adhesive". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.770 - 3.20 g/ccAverage value: 1.23 g/cc Grade Count:201
Volatile Organic Compounds (VOC) Content 0.000 - 510 g/lAverage value: 170 g/l Grade Count:17
Water Absorption 0.0600 - 0.400 %Average value: 0.214 % Grade Count:29
Moisture Absorption at Equilibrium 0.150 - 0.180 %Average value: 0.157 % Grade Count:4
Water Absorption at Saturation 0.00150 - 0.0120 %Average value: 0.00427 % Grade Count:17
Loss On Ignition 0.0500 - 0.570 %
@Temperature 100 - 130 °C
Average value: 0.304 % Grade Count:4
 0.0500 - 0.570 %
@Time 86400 - 605000 sec
Average value: 0.304 % Grade Count:4
Viscosity 30.0 - 1.20e+6 cPAverage value: 34700 cP Grade Count:164
 50.0 - 600000 cP
@Temperature 27.0 - 82.0 °C
Average value: 173000 cP Grade Count:10
Viscosity Measure 150 - 300000 cStAverage value: 77800 cSt Grade Count:11
Linear Mold Shrinkage 0.00100 - 0.0125 cm/cmAverage value: 0.00843 cm/cm Grade Count:20
Outgassing - Total Mass Loss 0.150 - 2.50 %Average value: 0.516 % Grade Count:16
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 10.0 - 103Average value: 63.8 Grade Count:147
 75.0 - 75.0
@Temperature -40.0 - -40.0 °C
Average value: 75.0 Grade Count:2
Hardness, Shore D 10.0 - 85.0Average value: 57.3 Grade Count:40
Hardness, Shore OO 50.0 - 65.0Average value: 61.3 Grade Count:4
Tensile Strength, Ultimate 0.0392 - 39.3 MPaAverage value: 8.57 MPa Grade Count:152
Tensile Strength, Yield 0.0345 - 1.72 MPaAverage value: 0.707 MPa Grade Count:10
Elongation at Break 9.00 - 874 %Average value: 345 % Grade Count:162
Elongation at Yield 68.0 - 250 %Average value: 204 % Grade Count:4
Modulus of Elasticity 0.0000345 - 1.93 GPaAverage value: 0.113 GPa Grade Count:39
 0.00413685 - 0.00413685 GPa
@Temperature 55.0 - 55.0 °C
Average value: 0.00414 GPa Grade Count:1
Compressive Yield Strength 0.0345 - 193 MPaAverage value: 27.4 MPa Grade Count:4
Compressive Modulus 0.000414 - 1.21 GPaAverage value: 0.405 GPa Grade Count:3
Shear Modulus 0.000800 - 0.00350 GPaAverage value: 0.00191 GPa Grade Count:57
Shear Strength 0.352 - 19.7 MPaAverage value: 4.65 MPa Grade Count:9
 0.690 - 17.2 MPa
@Temperature -55.0 - 121 °C
Average value: 5.90 MPa Grade Count:4
Adhesive Bond Strength 0.138 - 20.7 MPaAverage value: 4.95 MPa Grade Count:65
Tear Strength 6.14 - 132 kN/mAverage value: 49.4 kN/m Grade Count:10
Peel Strength 0.877 - 11.4 kN/mAverage value: 6.43 kN/m Grade Count:5
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00500 - 2.00e+16 ohm-cmAverage value: 1.52e+15 ohm-cm Grade Count:116
 1.30e+10 - 1.70e+15 ohm-cm
@Temperature 18.0 - 130 °C
Average value: 2.17e+14 ohm-cm Grade Count:10
Surface Resistance 3.50e+6 - 6.10e+17 ohmAverage value: 4.56e+16 ohm Grade Count:20
Insulation Resistance 2.40e-11 - 4.50e+14 ohmAverage value: 1.23e+14 ohm Grade Count:18
Dielectric Constant 1.51 - 7.90Average value: 3.83 Grade Count:73
 3.18 - 3.50
@Temperature -40.0 - 140 °C
Average value: 3.34 Grade Count:1
 3.18 - 3.50
@Frequency 1.00e+6 - 1.00e+6 Hz
Average value: 3.34 Grade Count:1
Dielectric Strength 0.600 - 138 kV/mmAverage value: 35.0 kV/mm Grade Count:60
Dielectric Breakdown 1500 VAverage value: 1500 V Grade Count:7
Dissipation Factor 0.00600 - 0.200Average value: 0.0408 Grade Count:65
 0.00500 - 0.0700
@Temperature -40.0 - 140 °C
Average value: 0.0375 Grade Count:1
 0.00500 - 0.0700
@Frequency 1.00e+6 - 1.00e+6 Hz
Average value: 0.0375 Grade Count:1
Arc Resistance 120 - 190 secAverage value: 124 sec Grade Count:18
 
Thermal PropertiesOriginal ValueComments
CTE, linear 1.00 - 510 µm/m-°CAverage value: 169 µm/m-°C Grade Count:52
 65.0 - 120 µm/m-°C
@Temperature 33.0 - 6.00 °C
Average value: 90.2 µm/m-°C Grade Count:6
Thermal Conductivity 0.100 - 1.76 W/m-KAverage value: 0.516 W/m-K Grade Count:34
Maximum Service Temperature, Air 51.7 - 160 °CAverage value: 106 °C Grade Count:147
Minimum Service Temperature, Air -90.0 - -30.0 °CAverage value: -45.7 °C Grade Count:136
Glass Transition Temp, Tg -83.0 - 71.0 °CAverage value: -31.6 °C Grade Count:47
Flash Point -1.11 - 200 °CAverage value: 91.3 °C Grade Count:58
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90.0 - 93.4 %Average value: 90.3 % Grade Count:10
 
Processing PropertiesOriginal ValueComments
Processing Temperature -40.0 - 125 °CAverage value: 52.4 °C Grade Count:102
Cure Time 15.0 - 43200 minAverage value: 5150 min Grade Count:66
 5.00 - 20160 min
@Temperature 60.0 - 190 °C
Average value: 1090 min Grade Count:47
Tack-Free Time 4.00 - 480 minAverage value: 71.0 min Grade Count:34
Pot Life 1.00 - 600 minAverage value: 34.9 min Grade Count:107
 0.750 - 50.0 min
@Temperature 32.0 - 120 °C
Average value: 16.9 min Grade Count:3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Epoxy Adhesive
Overview of materials for Cyanoacrylate Adhesive
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
Overview of materials for Epoxy Adhesive, Flexible
Overview of materials for Epoxy Cure Resin

O5003 / 78454

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.