MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

The Chemical Company Nature-Flexx 509 Acetyl Tributyl Citrate, C20H34O8
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: NatureFlexx 509 plasticizer or Acetyl Tri-n-Butyl Citrate (ATBC), a tributyl ester, is an innocuous plasticizer of PVC, cellulose resin and synthetic rubber. The chemical compound is used to fulfill plastic industry needs for non-toxic plasticizers that provide flexibility in soft toys for children, medical products such as blood bags, food packaging materials, and cosmetics.
The liquid chemical is a colorless organic compound belonging to the carboxylic acid family. It exists in all plants, particularly lemons and limes as well as in many animal tissues and fluids.
Molecular Formula: C20H34O8

Information provided by The Chemical Company

Key Words: ATBC;CAS Number 77-90-7
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.045 - 1.055 g/cc
@Temperature 25.0 °C
1.045 - 1.055 g/cc
@Temperature 77.0 °F
(25/25°C)
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 0.20<= 0.20mg KOH/gm
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.441 - 1.44251.441 - 1.4425(25°C/D)
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.15 %<= 0.15 %Weight percent
 
Component Elements PropertiesMetricEnglishComments
Arsenic, As <= 0.00030 %<= 0.00030 %
Lead, Pb <= 0.0010 %<= 0.0010 %Heavy metal content
 
Descriptive Properties
AppearanceColorless Transparent Liquid
Assay= 99.0%
Hazen Color Value (pt-co)= 30

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lanxess PUROLAN® BC Tributyl Citrate Plasticizer
Overview of materials for Nylon 12
Overview of materials for Nylon 12, Glass Bead Filled
Overview of materials for Nylon 12, PTFE Filled
Overview of materials for Nylon 12, Carbon Fiber Filled

PTCC002 / 106991

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.