MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M Panagraphics™ III Wide Width Flexible Substrate
Categories: Polymer; Film

Material Notes: 22 mil white-pigmented vinyl substrate with a polyester scrim; Smooth front surface with a semi-gloss finish; Decorate first or second surface with inkjet direct printing or first surface with cut film before or after attaching to mounting devices; Wide, long widths available for seamless backlit signs; Medium to long-term durability; Cost effective

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Brightness >= 100 %>= 100 %Whiteness
Thickness 533 - 584 microns21.0 - 23.0 mil
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 47.0 MPa6820 psiweft
 47.0 MPa6820 psiwarp
Tear Strength 13.1 kN/m75.1 pliwarp
 14.9 kN/m85.1 pliweft
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 70.0 °C158 °F
Minimum Service Temperature, Air -30.0 °C-22.0 °F
 
Optical PropertiesMetricEnglishComments
Gloss 30 %30 %60°
Transmission, Visible 19 - 23 %19 - 23 %
 
Processing PropertiesMetricEnglishComments
Processing Temperature >= 7.00 °C>= 44.6 °FApplication Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM34836 / 169583

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.