MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Elexar® EL 1934E Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Elexar® EL-1934E is a high performance UL V-0 flame retardant thermoplastic elastomer designed for electrical applications requiring flexibility over a wide temperature range. Elexar EL-1934E is a high hardness, high density, high flow grade that is UV stabilized and RoHS compliant. This UL listed grade is easily colorable and is suitable for both molding and extrusion.

Features: : Chemical Resistant; Flame Retardant; General Purpose; Good Adhesion; Good Colorability; Good Flexibility; Good Toughness; Halogenated; High Density; High Hardness; High Specific Gravity; Low Flow; Slip; Sunlight Resistant (720 hours); UV Resistant

Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; General Purpose; Industrial Applications; Industrial Cable Insulation; Rubber Replacement; Terminal Cable Jacketing; Underground Power Cable; Wire & Cable Applications; Wire Jacketing

Form: Pellets

Processing Method: Extrusion; Injection Molding

Information Provided by Teknor Apex

Key Words: TPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.31 g/ccASTM D792
Moisture Absorption at Equilibrium <= 1.0 %ASTM D570
Melt Flow 7.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80
@Time 5.00 sec
ASTM D2240
 81
@Time 1.00 sec
ASTM D2240
Tensile Strength at Break 9.10 MPaASTM D412
 8.58 MPa
@Treatment Temp. 60.0 °C,
Time 605000 sec
in IRM 902 Oil; ASTM D471
 8.79 MPa
@Treatment Temp. 136 °C,
Time 605000 sec
in Air; ASTM D573
Tensile Stress at Strain 457 psi
@Strain 100 %
ASTM D412
 632 psi
@Strain 300 %
ASTM D412
Elongation at Break 620 %ASTM D412
 598.92 %
@Treatment Temp. 60.0 °C,
Time 605000 sec
in IRM 902 Oil; ASTM D471
 634.88 %
@Treatment Temp. 136 °C,
Time 605000 sec
in Air; ASTM D573
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 4.10e+14 ohm-cm122°F; ASTM D257
Dielectric Constant 2.47
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 1100 V/milASTM D419
Dissipation Factor 0.0030ASTM D150
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 221 °CUL 1581
Brittleness Temperature -51.5 °CASTM D746
UL RTI, Electrical 122 °FUL 746
UL RTI, Mechanical with Impact 50.0 °CUL 746
UL RTI, Mechanical without Impact 50.0 °CUL 746
Flammability, UL94 V-00.05 to 0.06 in, All Colors
Oxygen Index 30 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 390 - 420 °F
Middle Barrel Temperature 415 - 430 °F
Front Barrel Temperature 430 - 440 °F
Nozzle Temperature 430 - 445 °F
Zone 1 380 - 410 °F
Zone 2 390 - 420 °F
Zone 3 415 - 430 °F
Zone 4 415 - 430 °F
Zone 5 430 - 440 °F
Melt Temperature 430 - 445 °FProcessing Temp
Mold Temperature 77.0 - 150 °F
Injection Pressure 200 - 1000 psi
Back Pressure 25.0 - 50.0 psi
Cushion 0.150 - 1.00 in
Screw Speed 50 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient OnFlex™ S KE 50A-3S1731 Thermoplastic Elastomer (TPE)
Advanced Elastomer Systems Santoprene® 101-64 W175 Thermoplastic Rubber
ExxonMobil Santoprene® 101-55W185 Thermoplastic Elastomer
Huntsman IROGRAN® A 78 P 4766 NM Ether-Based TPU-For Cable Industry
Teknor Apex Telcar® TL-1934F Styrenic Thermoplastic Elastomer

PTEKNO773 / 128954

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.