MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Perstorp Compounds AMITEC 751 Melamine
Categories: Polymer; Thermoset; Melamine; Melamine Formaldehyde, Molded, Unreinforced

Material Notes: Perstorp dinnerware compression and injection grade. Porcelain like properties suitable for household applications.

Information provided by Perstorp Compounds Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cmDIN 53 464
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break >= 45.0 MPaISO 178
Flexural Strength >= 80.0 MPaISO 178
Charpy Impact Unnotched >= 0.500 J/cm²1eU; ISO 179
Charpy Impact, Notched >= 0.110 J/cm²1eU; ISO 179
 
Electrical PropertiesOriginal ValueComments
Surface Resistance >= 1.00e+11 ohmDIN 53 482
Dielectric Constant 5.0DIN 53 483
Comparative Tracking Index >= 500 VIEC 112
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) >= 155 °CISO 175
Deflection Temperature at 8.0 MPa >= 110 °CISO 175
Flammability, UL94 V-0
Oxygen Index >= 40 %ASTM D2863
Shrinkage 1.5 - 1.8 %Post Shrinkage; DIN 53 464
 
Descriptive Properties
Acetic Acid Fa Emission>3 mg/lDIN 7708
Ethanol Fa Emission>3 mg/lDIN 7708
Glow Bar 960°C 180 secpassesIEC 707
H2O Fa Emission>3 mg/lDIN 7708
Water Absorption [mg]<200DIN 53 495/23°C 96h

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Elektro-Isola G-Etronax M Melamine, Glass Fabric Reinforcement, White, Sheets
Perstorp Compounds Aminel GF Melamine
Hippe MF GC 21 Woven Glass Cloth Reinforced Melamine Resin - Round, Rolled Tube
Hippe MF GC 201 Woven Glass Cloth Reinforced Melamine Resin - Sheet
Perstorp Compounds Aminel FX Melamine

PPERST09 / 56186

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.