MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

A. Schulman POLYFLAM™ FLP 3714 20% Glass Filled HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Glass fiber Filled

Material Notes: Description

Polyfort® FLP 3714 is a 20% glass filled HDPE product.

Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccASTM D792
Melt Flow 10 g/10 min10 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 35.0 MPa5080 psiASTM D638
Elongation at Break 2.0 %2.0 %ASTM D638
Flexural Strength 43.0 MPa6240 psiASTM D790
Flexural Modulus 2.80 GPa406 ksiASTM D790
Izod Impact, Notched 0.570 J/cm1.07 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 123 °C253 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 102 °C216 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aclo Accutech Polyethylene HD0204UVL High Density UV Stabilized
Aclo Accutech Polyethylene HD0234G10UVL High Density Glass Reinforced UV Stabilized
RTP Company RTP 100 GB 20 Polypropylene (PP), Glass Bead
RTP Company RTP 705 UV  High Density Polyethylene (HDPE) Glass Fiber 30% - UV Stable
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled

PASHU107 / 25071

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.