MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Iodine, I2
Categories: Pure Element

Key Words: I2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.933 g/cc0.1782 lb/in³
Molecular Weight 253.809 g/mol253.809 g/mol
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 126.9045126.9045126.90447 - 1995
Atomic Number 5353
X-ray Absorption Edge 0.373 Å0.373 ÅK
 2.38982 Å2.38982 ÅLI
 2.55324 Å2.55324 ÅLII
 2.71901 Å2.71901 ÅLIII
Critical Temperature 546 °C1010 °F
Electronegativity 2.662.66Pauling
Ionic Radius 0.500 Å0.500 ÅCrystal Ionic Radius for Valence +7
 0.620 Å0.620 ÅCrystal Ionic Radius for Valence +5
 2.20 Å2.20 ÅCrystal Ionic Radius for Valence -1
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 61.1 J/g26.3 BTU/lb
Specific Heat Capacity 0.145 J/g-°C0.0347 BTU/lb-°F
Melting Point 113.7 °C236.7 °F
Boiling Point 184.4 °C363.9 °F
 
Component Elements PropertiesMetricEnglishComments
Iodine, I 100 %100 %
 
Descriptive Properties
AppearanceBlue-Black Plates
CAS Number7553-56-2
Crystal StructureRhombic

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Silicon Dioxide, SiO2 (Alpha Quartz)
Holmium, Ho
Lutetium, Lu
Cesium Iodide, CsI
Cesium Hydroxide, CsOH

AMEI00 / 3473

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.