MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 6004-45A Specialty Thermoplastic Elastomer, designed for overmolding onto nylon 6 substrates
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: 45 Shore A thermoplastic elastomer designed for overmolding onto nylon 6 substrates.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.980 g/cc0.980 g/ccASTM D 792
Linear Mold Shrinkage 0.013 - 0.017 cm/cm
@Thickness 3.20 mm
0.013 - 0.017 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 51
@Time 10.0 sec
51
@Time 0.00278 hour
ASTM D 2240
Tensile Strength at Break 2.76 MPa
@Thickness 3.20 mm
400 psi
@Thickness 0.126 in
Die C; 20 in/min (500 mm/min); ASTM D 412
Elongation at Break 300 %
@Thickness 3.20 mm
300 %
@Thickness 0.126 in
Die C, 20 in/min (500 mm/min); ASTM D 412
Tear Strength 14.0 kN/m80.0 pliDie C; ASTM D 624
Peel Strength 3.16 kN/m18.0 pli90 degrees, 20 in/min (500 mm/min); vs. Nylon 6; Failure Type D; ISO 813
 
Processing PropertiesMetricEnglishComments
Melt Temperature 216 - 249 °C420 - 480 °F
Mold Temperature 48.9 - 65.6 °C120 - 150 °F
Drying Temperature 79.4 °C
@Time 7200 - 10800 sec
175 °F
@Time 2.00 - 3.00 hour
Moisture Content <= 0.030 %<= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PQZUA9631 / 134912

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.