MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trelleborg Horda Cable E8400 Easy Strippable Semiconductive Shielding
Categories: Polymer; Thermoset

Material Notes: E8400 is a vulcanizable, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.

E8400 meets these requirements when optimal processing, extrusion, and end testing procedure are used:
AEIC-CS 5/94
BS 6622
HN 33-S-23 (EDF)
IEC 502
IEC 840
NF CS 32/321
SS 424 14 16, SS 424 14 17 (HD 620 S1:1996)
VDE 0273 / 12.87

All information provided by Horda Cable Compounds

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/cc
@Temperature 23.0 °C
ASTM D1928
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 85 - 90ASTM D2240
Tensile Strength, Yield 12.35 MPaafter aging 1 week @ 135°C; ASTM D638
 13.0 MPaASTM D638
Elongation at Break 150 %after aging 1 week @ 135°C; ASTM D638
 250 %ASTM D638
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 500 ohm-cm
@Temperature 23.0 °C
ASTM D257
 <= 1000 ohm-cm
@Temperature 90.0 °C
ASTM D257
 <= 1000 ohm-cm
@Temperature 120 °C
ASTM D257
 
Processing PropertiesOriginal ValueComments
Middle Barrel Temperature 60.0 - 110 °C
Head Temperature 100 - 130 °C
Screw Cooling Temperature 40.0 - 50.0 °C
Drying Temperature <= 40.0 °C
Moisture Content <= 0.080 %QAHC-10420 (Karl Fischer method)
 
Descriptive Properties
Hot Set (%)20/5200°C, 20 N/cm²; IEC 540
Insulation Shield Stripping Force (N/cm)8-14@ 90°

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trelleborg E450 EPDM Rubber
Top Polymer Topolymer® 9210-851 Thermoplastic Vulcanized Elastomer
Top Polymer Topolymer® 9210-801 Thermoplastic Vulcanized Elastomer
Top Polymer Topolymer® 9210-751 Thermoplastic Vulcanized Elastomer
Top Polymer Topolymer® 9210-651 Thermoplastic Vulcanized Elastomer

PTRELL014 / 83772

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.